Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.5 g/cm³ Show Supplier Material materials with Dichte of 1.5 g/cm³ | ASTM D 792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 351 MPa Show Supplier Material materials with Biegefestigkeit of 351 MPa | ASTM D 790 |
Biegemodul | 23.0 °C | 18.6 GPa Show Supplier Material materials with Biegemodul of 18.6 GPa | ASTM D 790 |
Dehnung | 23.0 °C | 0.9 % Show Supplier Material materials with Dehnung of 0.9 % | ASTM D 638 | break |
Elastizitätsmodul | 23.0 °C | 27 GPa Show Supplier Material materials with Elastizitätsmodul of 27 GPa | ASTM D 638 | 50 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 78 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 78 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 1018 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 1018 J/m | ASTM D 4812 | 23°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 78 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 78 kJ/m² | ASTM D 256 | notched, 23°C |
Zugfestigkeit | 23.0 °C | 228 MPa Show Supplier Material materials with Zugfestigkeit of 228 MPa | ASTM D 638 | break |
Thermisch
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 10 - 10000 Ω Show Supplier Material materials with Sheet resistivity, ROA of 10 - 10000 Ω | ASTM D 257 |
Technological properties
Property | ||
---|---|---|
Application areas | Wireless Communications, Enclosures | |
Availability | Asia,Americas | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |