Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.26 g/cm³ Show Supplier Material materials with Dichte of 1.26 g/cm³ | ASTM D 792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 84 MPa Show Supplier Material materials with Biegefestigkeit of 84 MPa | ASTM D 790 |
Biegemodul | 23.0 °C | 2.2 GPa Show Supplier Material materials with Biegemodul of 2.2 GPa | ASTM D 790 |
Dehnung | 23.0 °C | 5 % Show Supplier Material materials with Dehnung of 5 % | ASTM D 638 | yield |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 640 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 640 kJ/m² | ASTM D 256 | notched, 23°C |
Zugfestigkeit | 23.0 °C | 49 MPa Show Supplier Material materials with Zugfestigkeit of 49 MPa | ASTM D 638 | break |
Thermisch
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 1.00E+10 - 1.00E+12 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+10 - 1.00E+12 Ω | ASTM D 257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 0.53 % Show Supplier Material materials with Schrumpfung of 0.53 % | ASTM D 955 | 24 hrs |
Technological properties
Property | ||
---|---|---|
Application areas | Rail Cabin Interiors, Monitoring and Imaging, Personal Computing, Document Handling, Data Management, Lab Ware and Clinical Diagnostics, Electronic Components | |
Availability | Europe,Asia,Americas | |
Processing methods | Front - Zone 3 Temperature: 220 to 230.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |