Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.6 g/cm³ Show Supplier Material materials with Dichte of 1.6 g/cm³ | ASTM D 792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 178 MPa Show Supplier Material materials with Biegefestigkeit of 178 MPa | ISO 178 | break, 2 mm/min |
Biegemodul | 23.0 °C | 9.7 GPa Show Supplier Material materials with Biegemodul of 9.7 GPa | ISO 178 |
Dehnung | 23.0 °C | 1.8 % Show Supplier Material materials with Dehnung of 1.8 % | ISO 527 | break, 5 mm/min |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 8 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 8 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Schlagzähigkeit, Izod ungekerbt | 23.0 °C | 40 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod ungekerbt of 40 kJ/m² | ISO 180/1U | 80*10*4, 23°C |
Zugfestigkeit | 23.0 °C | 127 MPa Show Supplier Material materials with Zugfestigkeit of 127 MPa | ISO 527 | break, 5 mm/min |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 211 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 211 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |
Relative temperature index, electrical | 190 °C Show Supplier Material materials with Relative temperature index, electrical of 190 °C | UL 746B | |
Relative temperature index, mechanical impact | 190 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 190 °C | UL 746B | |
Relative temperature index, mechanical strength | 190 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 190 °C | UL 746B | |
Wärmeformbeständigkeitstemperatur | 211 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 211 °C | ||
Entflammbarkeit | UL Recognized, 94V-0 Flame Class Rating: 0.5mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101283894- - |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 0.3 % Show Supplier Material materials with Schrumpfung of 0.3 % | ASTM D 955 | 24 hrs |
Technological properties
Property | ||
---|---|---|
Application areas | Meter Water | |
Availability | Europe,Americas | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |