Allgemein
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 98 MPa Show Supplier Material materials with Biegefestigkeit of 98 MPa | ISO 178 | yield, 2 mm/min |
Biegemodul | 23.0 °C | 6.2 GPa Show Supplier Material materials with Biegemodul of 6.2 GPa | ISO 178 | 2 mm/min |
Dehnung | 23.0 °C | 2.8 % Show Supplier Material materials with Dehnung of 2.8 % | ISO 527 | yield, 5 mm/min |
Elastizitätsmodul | 23.0 °C | 5.6 GPa Show Supplier Material materials with Elastizitätsmodul of 5.6 GPa | ISO 527 | 1 mm/min |
Hardness, Rockwell R | 23.0 °C | 109 [-] Show Supplier Material materials with Hardness, Rockwell R of 109 [-] | ASTM D 785 |
Impact strength, Izod notched, ASTM | 23.0 °C | 50 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 50 J/m | ASTM D 256 |
Instrumented Impact, Total Energy | 23.0 °C | 20 J Show Supplier Material materials with Instrumented Impact, Total Energy of 20 J | ASTM D 3763 | 23°C |
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 6 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 6 kJ/m² | ISO 179/1eA | V-notch Edgew, 23°C, 80*10*4 sp=62mm |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 50 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 50 kJ/m² | ASTM D 256 | notched, 23°C |
Zugfestigkeit | 23.0 °C | 30 MPa Show Supplier Material materials with Zugfestigkeit of 30 MPa | ISO 527 | break, 5 mm/min |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Heat deflection temperature, 0.45 MPa | 93 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 93 °C | ASTM D 648 | 3.2 mm, unannealed | |||
Heat deflection temperature, 1.80 MPa | 87 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 87 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 3.4E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 3.4E-5 1/K | ISO 11359-2 | 23°C to 80°C | ||
Relative temperature index, electrical | 80 °C Show Supplier Material materials with Relative temperature index, electrical of 80 °C | UL 746B | |||
Relative temperature index, mechanical impact | 80 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 80 °C | UL 746B | |||
Relative temperature index, mechanical strength | 80 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 80 °C | UL 746B | |||
Vicat-Erweichungstemperatur | 98 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 98 °C | ASTM D 1525 | Rate B/50 | |||
Wärmeformbeständigkeitstemperatur | 87 - 93 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 87 - 93 °C | ||||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 6.9E-5 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 6.9E-5 1/K | ISO 11359-2 | 23°C to 80°C | ||
Entflammbarkeit | UL Recognized, 94V-0 Flame Class Rating: ≥1.2mm UL 94 <br> UL Recognized, 94-5VB Flame Class Rating: ≥1.5mm UL 94 <br> UL Recognized, 94V-1 Flame Class Rating: ≥0.8mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101901446- - |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzmassenflussrate | 12 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 12 g/10min | ASTM D 1238 | 260°C/2.16 kgf | |
Schrumpfung | 23.0 °C | 0.3 % Show Supplier Material materials with Schrumpfung of 0.3 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Personal Computing, Data Management | |
Availability | Asia | |
Processing methods | Front - Zone 3 Temperature: 270 to 290.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |