Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.25 g/cm³ Show Supplier Material materials with Dichte of 1.25 g/cm³ | ISO 1183 |
Moisture absorption | 23.0 °C | 0.04 % Show Supplier Material materials with Moisture absorption of 0.04 % | ISO 62 | (23°C / 50% RH) |
Relative Dichte | 23.0 °C | 1.25 [-] Show Supplier Material materials with Relative Dichte of 1.25 [-] | ASTM D 792 |
Wasserabsorption | 23.0 °C | 0.13 % Show Supplier Material materials with Wasserabsorption of 0.13 % | ISO 62-1 | (23°C/saturated) |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 87 MPa Show Supplier Material materials with Biegefestigkeit of 87 MPa | ASTM D 790 | yld, 1.3 mm/min, 50 mm span |
Biegemodul | 23.0 °C | 3.6 GPa Show Supplier Material materials with Biegemodul of 3.6 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Dehnung | 23.0 °C | 11 % Show Supplier Material materials with Dehnung of 11 % | ASTM D 638 | brk, Type I, 5 mm/min |
Elastizitätsmodul | 23.0 °C | 3.9 GPa Show Supplier Material materials with Elastizitätsmodul of 3.9 GPa | ASTM D 638 | 5 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 205 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 205 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 1880 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 1880 J/m | ASTM D 4812 | 23°C |
Instrumented Impact, Total Energy | 23.0 °C | 36 J Show Supplier Material materials with Instrumented Impact, Total Energy of 36 J | ASTM D 3763 | 23°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 205 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 205 kJ/m² | ASTM D 256 | notched, 23°C |
Zugfestigkeit | 23.0 °C | 37 MPa Show Supplier Material materials with Zugfestigkeit of 37 MPa | ASTM D 638 | brk, Type I, 5 mm/min |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 0.45 MPa | 127 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 127 °C | ASTM D 648 | 3.2 mm, unannealed | |
Heat deflection temperature, 1.80 MPa | 120 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 120 °C | ASTM D 648 | 3.2mm, unannealed | |
Relative temperature index, electrical | 80 °C Show Supplier Material materials with Relative temperature index, electrical of 80 °C | UL 746B | |
Relative temperature index, mechanical impact | 80 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 80 °C | UL 746B | |
Relative temperature index, mechanical strength | 80 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 80 °C | UL 746B | |
Vicat-Erweichungstemperatur | 132 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 132 °C | ISO 306 | Rate B/120 | |
Wärmeformbeständigkeitstemperatur | 120 - 127 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 120 - 127 °C | ||
Entflammbarkeit | UL Recognized, 94HB Flame Class Rating: ≥0.4mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101619221- - |
Optisch
Property | Value | Comment |
---|---|---|
Transmission | -2.5 % Show Supplier Material materials with Transmission of -2.5 % | <, SABIC method | at 0.4 mm |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzmassenflussrate | 15 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 15 g/10min | ASTM D 1238 | 300°C/1.2 kgf | |
Schmelzvolumenflussrate | 14 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 14 cm³/10min | ISO 1133 | MVR at 300°C/1.2 kg | |
Schrumpfung | 23.0 °C | 0.2 % Show Supplier Material materials with Schrumpfung of 0.2 % | SABIC method | 3.2 mm |
Schrumpfung, diagonal | 23.0 °C | 0.4 % Show Supplier Material materials with Schrumpfung, diagonal of 0.4 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Enclosures, Personal Computing, Photo/Video Camera, Wireless Communications | |
Availability | Asia | |
Processing methods | Vent Depth: 0.025 to 0.076mm | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |