NORYL™ Resin HNA055 - Asia

Want to keep this datasheet? Save it now in your required format

Description

NORYL™ HNA055 resin is a non-reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This injection moldable grade was designed to withstand extended duty high heat autoclave sterilization >2500 cycles and exhibits good chemical resistance to lipids and typical hospital cleansers. In additional, this grade is US FDA Food Contact approved, biocompatible (ISO10993 or USP Class VI), RoHS compliant, and it is subject to SABIC’s Healthcare management of change and formulation lock. NORYL HNA055 resin may be an excellent candidate for applications requiring extended duty sterilization cycles such as sterilization trays, dental trays, surgical instrument handles, and animal cages.

Diese Materialdaten wurden von Sabic zur Verfügung gestellt

Alle Daten beziehen sich auf Raumtemperatur soweit nicht anderweitig spezifiziert. SI Einheiten werden verwendt soweit nicht anderweitig spezifiziert.
Äquivalente Standards sind ähnlich zu einem oder mehreren Standards die der Anbieter angegeben hat. Manche äquivalente Standards können strikter sein oder außerhalb der Bedingungen des ursprünglichen Standards.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Eigenschaften

Allgemein

PropertyTemperatureValueComment

Dichte

23.0 °C

1.08 g/cm³

Show Supplier Material materials with Dichte of 1.08 g/cm³

ISO 1183

Moisture absorption

23.0 °C

0.06 %

Show Supplier Material materials with Moisture absorption of 0.06 %

ISO 62 | (23°C / 50% RH)

Relative Dichte

23.0 °C

1.08 [-]

Show Supplier Material materials with Relative Dichte of 1.08 [-]

ASTM D 792

Wasserabsorption

23.0 °C

0.23 %

Show Supplier Material materials with Wasserabsorption of 0.23 %

ISO 62-1 | (23°C/saturated)

Mechanisch

PropertyTemperatureValueComment

Biegefestigkeit

23.0 °C

107 MPa

Show Supplier Material materials with Biegefestigkeit of 107 MPa

ISO 178 | yield, 2 mm/min

Biegemodul

23.0 °C

2.5 GPa

Show Supplier Material materials with Biegemodul of 2.5 GPa

ISO 178 | 2 mm/min

Dehnung

23.0 °C

12.6 %

Show Supplier Material materials with Dehnung of 12.6 %

ISO 527 | break, 50 mm/min

Elastizitätsmodul

23.0 °C

2.4 GPa

Show Supplier Material materials with Elastizitätsmodul of 2.4 GPa

ISO 527 | 1 mm/min

Impact strength, Izod notched, ASTM

23.0 °C

144 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM of 144 J/m

ASTM D 256

Instrumented Impact, Total Energy

23.0 °C

54 J

Show Supplier Material materials with Instrumented Impact, Total Energy of 54 J

ASTM D 3763 | 23°C

Schlagfestigkeit, Charpy gekerbt

23.0 °C

27 kJ/m²

Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 27 kJ/m²

ISO 179/1eA | V-notch Edgew 80*10*4 sp=62mm, 23°C

Schlagzähigkeit, Izod gekerbt

23.0 °C

24 kJ/m²

Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 24 kJ/m²

ISO 180/1A | notched 80*10*4, 23°C

Zugfestigkeit

23.0 °C

57 MPa

Show Supplier Material materials with Zugfestigkeit of 57 MPa

ISO 527 | break, 50 mm/min

Thermisch

PropertyTemperatureValueComment

Heat deflection temperature, 1.80 MPa

147 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 147 °C

ISO 75/Af | Flatw 80*10*4 sp=64mm

Koeffizient der thermischen Ausdehnung

23.0 °C

8.66E-5 1/K

Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 8.66E-5 1/K

ISO 11359-2 | -40°C to 40°C

Vicat-Erweichungstemperatur

169 °C

Show Supplier Material materials with Vicat-Erweichungstemperatur of 169 °C

ISO 306 | Rate B/120

Wärmeformbeständigkeitstemperatur

147 °C

Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 147 °C

thermischer Ausdehnungskoeffizient, transversal

23.0 °C

9.25E-5 1/K

Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 9.25E-5 1/K

ISO 11359-2 | -40°C to 40°C

Rheological Properties

PropertyTemperatureValueComment

Schmelzmassenflussrate

6.2 g/10min

Show Supplier Material materials with Schmelzmassenflussrate of 6.2 g/10min

ASTM D 1238 | 300°C/5.0 kgf

Schmelzvolumenflussrate

5 cm³/10min

Show Supplier Material materials with Schmelzvolumenflussrate of 5 cm³/10min

ISO 1133 | MVR at 300°C/5.0 kg

Schrumpfung

23.0 °C

0.6 %

Show Supplier Material materials with Schrumpfung of 0.6 %

SABIC method | 3.2 mm

Technological properties

Property
Application areas

Fluid Delivery, Lab Ware and Clinical Diagnostics, Enclosures, Surgical Tray, Toy, Tray, Wiring Devices, Surgical Devices, Respiratory, Medical Device, Monitoring and Imaging, Medical Facility Infrastructure

Availability

Europe,Asia,Americas

Processing methods

Nozzle Temperature: 295 to 315.0°C
Front - Zone 3 Temperature: 280 to 315.0°C
Drying Time: 3 to 4.0hrs
Drying Time (Cumulative): 8hrs
Drying Temperature: 105 to 110.0°C
Screw Speed: 20 to 100.0rpm
Melt Temperature: 295 to 315.0°C
Rear - Zone 1 Temperature: 260 to 305.0°C
Middle - Zone 2 Temperature: 270 to 310.0°C
Maximum Moisture Content: 0.02%
Shot to Cylinder Size: 30 to 70.0%
Mold Temperature: 75 to 105.0°C
Back Pressure: 0.3 to 0.7MPa

Supplier Disclaimer

While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right.