Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of friction | 0.41 - 0.46 [-] Show Supplier Material materials with Coefficient of friction of 0.41 - 0.46 [-] | ||
Coefficient of friction, kinetic | 0.46 [-] Show Supplier Material materials with Coefficient of friction, kinetic of 0.46 [-] | ASTM D 3702 Modified: Manual | |
Coefficient of friction, static | 0.41 [-] Show Supplier Material materials with Coefficient of friction, static of 0.41 [-] | ASTM D 3702 Modified: Manual | |
Dichte | 23.0 °C | 1.54 g/cm³ Show Supplier Material materials with Dichte of 1.54 g/cm³ | ASTM D 792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 185 MPa Show Supplier Material materials with Biegefestigkeit of 185 MPa | ISO 178 |
Biegemodul | 23.0 °C | 8.3 GPa Show Supplier Material materials with Biegemodul of 8.3 GPa | ISO 178 |
Dehnung | 23.0 °C | 2.6 % Show Supplier Material materials with Dehnung of 2.6 % | ISO 527 | yield |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 16 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 16 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Schlagzähigkeit, Izod ungekerbt | 23.0 °C | 55 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod ungekerbt of 55 kJ/m² | ISO 180/1U | 80*10*4, 23°C |
Zugfestigkeit | 23.0 °C | 118 MPa Show Supplier Material materials with Zugfestigkeit of 118 MPa | ISO 527 | yield |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 143 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 143 °C | ASTM D 648 | 3.2mm, unannealed | |
Wärmeformbeständigkeitstemperatur | 143 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 143 °C | ||
Entflammbarkeit | UL Recognized, 94V-1 Flame Class Rating: ≥3mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101344609- - |
Technological properties
Property | ||
---|---|---|
Application areas | Small Appliance, Photovoltaic Components, Plumbing, Medical Device, Meter Water, Personal Computing, Document Handling, Displays, Data Management, Electronic Components, Lab Ware and Clinical Diagnostics | |
Availability | Europe,Americas | |
Processing methods | Middle - Zone 2 Temperature: 310 to 320.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |