Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Wasserabsorption | 23.0 °C | 0.16 % Show Supplier Material materials with Wasserabsorption of 0.16 % | ASTM D 570 | (23°C/24hrs) |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 137 MPa Show Supplier Material materials with Biegefestigkeit of 137 MPa | ASTM D 790 | yld, 2.6 mm/min, 100 mm span |
Biegemodul | 23.0 °C | 3.1 GPa Show Supplier Material materials with Biegemodul of 3.1 GPa | ASTM D 790 | 2.6 mm/min, 100 mm span |
Dehnung | 23.0 °C | 60 % Show Supplier Material materials with Dehnung of 60 % | ASTM D 638 | brk, Type I, 5 mm/min |
Elastizitätsmodul | 23.0 °C | 2.9 GPa Show Supplier Material materials with Elastizitätsmodul of 2.9 GPa | ASTM D 638 | 5 mm/min |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 64 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 64 kJ/m² | ASTM D 256 | notched, 23°C |
Zugfestigkeit | 23.0 °C | 99 MPa Show Supplier Material materials with Zugfestigkeit of 99 MPa | ASTM D 638 | yld, Type I, 5 mm/min |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 207 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 207 °C | ASTM D 648 | 6.4 mm, unannealed | |
Relative temperature index, electrical | 160 °C Show Supplier Material materials with Relative temperature index, electrical of 160 °C | UL 746B | |
Relative temperature index, mechanical impact | 160 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 160 °C | UL 746B | |
Relative temperature index, mechanical strength | 160 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 160 °C | UL 746B | |
Wärmeformbeständigkeitstemperatur | 207 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 207 °C | ||
Entflammbarkeit | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=221114- - <br> UL Recognized, 94V-0 Flame Class Rating: ≥1.5mm UL 94 |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Durchschlagfestigkeit | 23.0 °C | 17.9 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 17.9 kV/mm | ASTM D 149 | in oil, 3.2 mm |
High Amp Arc Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with High Amp Arc Ignition of 1.5 mm | ≥, UL 746A | PLC 0 |
High Volt Arc Track Rate | 23.0 °C | 3 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 3 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with Hot-Wire Ignition of 1.5 mm | ≥, UL 746A | PLC 0 |
Kriechstromfestigkeit | 23.0 °C | 4 V Show Supplier Material materials with Kriechstromfestigkeit of 4 V | UL 746A | (UL) {PLC} |
Sheet resistivity, ROA | 23.0 °C | 5.80E+16 Ω Show Supplier Material materials with Sheet resistivity, ROA of 5.80E+16 Ω | ASTM D 257 |
Volume resistivity | 23.0 °C | 1.10E+17 Ω·cm Show Supplier Material materials with Volume resistivity of 1.10E+17 Ω·cm | ASTM D 257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 0.4 % Show Supplier Material materials with Schrumpfung of 0.4 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Medical Device, LED Lighting, Meter Water, Photovoltaic Components, Semiconductor, Wireless Communications, Audio, Aerospace, Air Cabin Interiors, Electronic Components, Enclosure/Housing/Cover, Energy Management, Enclosures, Industrial Material Handling, Heavy Vehicles | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 150°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |