Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Wasserabsorption | 23.0 °C | 1.2 % Show Supplier Material materials with Wasserabsorption of 1.2 % | ISO 62-1 | (23°C/saturated) |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 110 MPa Show Supplier Material materials with Biegefestigkeit of 110 MPa | ISO 178 | yield, 2 mm/min |
Biegemodul | 23.0 °C | 2.5 GPa Show Supplier Material materials with Biegemodul of 2.5 GPa | ISO 178 | 2 mm/min |
Dehnung | 23.0 °C | 50 % Show Supplier Material materials with Dehnung of 50 % | ISO 527 | break, 50 mm/min |
Elastizitätsmodul | 23.0 °C | 3.2 GPa Show Supplier Material materials with Elastizitätsmodul of 3.2 GPa | ISO 527 | 1 mm/min |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 8 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 8 kJ/m² | ISO 180/1A | notched 80*10*4, -30°C |
Zugfestigkeit | 23.0 °C | 95 MPa Show Supplier Material materials with Zugfestigkeit of 95 MPa | ISO 527 | break, 50 mm/min |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 200 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 200 °C | ISO 75/Ae | Edgew 120*10*4 sp=100mm | |
Relative temperature index, electrical | 160 °C Show Supplier Material materials with Relative temperature index, electrical of 160 °C | UL 746B | |
Relative temperature index, mechanical impact | 160 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 160 °C | UL 746B | |
Relative temperature index, mechanical strength | 160 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 160 °C | UL 746B | |
Wärmeformbeständigkeitstemperatur | 200 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 200 °C | ||
Entflammbarkeit | UL Recognized, 94V-0 Flame Class Rating: ≥1.5mm UL 94 <br> Glow Wire Flammability Index 960°C, passes at: 3.2mm IEC 60695-2-12 <br> Glow Wire Flammability Index 960°C, passes at: 3.2mm IEC 60695-2-12 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=221114- - |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Durchschlagfestigkeit | 23.0 °C | 26 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 26 kV/mm | IEC 60243-1 | in oil, 1.6 mm |
High Amp Arc Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with High Amp Arc Ignition of 1.5 mm | ≥, UL 746A | PLC 0 |
High Volt Arc Track Rate | 23.0 °C | 3 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 3 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with Hot-Wire Ignition of 1.5 mm | ≥, UL 746A | PLC 0 |
Kriechstromfestigkeit | 23.0 °C | 4 V Show Supplier Material materials with Kriechstromfestigkeit of 4 V | UL 746A | (UL) {PLC} |
Sheet resistivity, ROA | 23.0 °C | 1.00E+15 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+15 Ω | >, IEC 60093 |
Volume resistivity | 23.0 °C | 1.00E+15 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+15 Ω·cm | IEC 60093 | |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 0.6 % Show Supplier Material materials with Schrumpfung of 0.6 % | SABIC method | on tensile bar |
Technological properties
Property | ||
---|---|---|
Application areas | Medical Device, LED Lighting, Meter Water, Photovoltaic Components, Semiconductor, Wireless Communications, Audio, Aerospace, Air Cabin Interiors, Electronic Components, Enclosure/Housing/Cover, Energy Management, Enclosures, Industrial Material Handling, Heavy Vehicles | |
Availability | Europe,Asia,Americas | |
Processing methods | Melt Temperature: 360 to 410.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |