Allgemein
Property | Temperature | Value |
---|---|---|
Sauerstoffindex | 23.0 °C | 46 % Show Supplier Material materials with Sauerstoffindex of 46 % |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 210 MPa Show Supplier Material materials with Biegefestigkeit of 210 MPa | ISO 178 | break, 2 mm/min |
Biegemodul | 23.0 °C | 6.5 GPa Show Supplier Material materials with Biegemodul of 6.5 GPa | ISO 178 | 2 mm/min |
Dehnung | 23.0 °C | 2 % Show Supplier Material materials with Dehnung of 2 % | ISO 527 | break, 5 mm/min |
Elastizitätsmodul | 23.0 °C | 6.8 GPa Show Supplier Material materials with Elastizitätsmodul of 6.8 GPa | ISO 527 | 1 mm/min |
Zugfestigkeit | 23.0 °C | 140 MPa Show Supplier Material materials with Zugfestigkeit of 140 MPa | ISO 527 | break, 5 mm/min |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 0.45 MPa | 210 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 210 °C | ISO 75/Be | Edgew 120*10*4 sp=100mm | |
Heat deflection temperature, 1.80 MPa | 205 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 205 °C | ISO 75/Ae | Edgew 120*10*4 sp=100mm | |
Relative temperature index, electrical | 170 °C Show Supplier Material materials with Relative temperature index, electrical of 170 °C | UL 746B | |
Relative temperature index, mechanical impact | 170 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 170 °C | UL 746B | |
Relative temperature index, mechanical strength | 170 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 170 °C | UL 746B | |
Vicat-Erweichungstemperatur | 223 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 223 °C | ISO 306 | Rate A/50 | |
Wärmeformbeständigkeitstemperatur | 205 - 210 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 205 - 210 °C | ||
Entflammbarkeit | UL Recognized, 94-5VA Flame Class Rating: ≥1.9mm UL 94 <br> Glow Wire Flammability Index 960°C, passes at: 3.2mm IEC 60695-2-12 <br> Glow Wire Flammability Index 960°C, passes at: 3.2mm IEC 60695-2-12 <br> UL Recognized, 94V-0 Flame Class Rating: ≥0.41mm UL 94 <br> UV-light, water exposure/immersion: F1- UL 746C <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=221093- - <br> UL Yellow Card Link 2: https://iq.ul.com/ul/cert.aspx?ULID=502535- - |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
High Amp Arc Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with High Amp Arc Ignition of 1.5 mm | ≥, UL 746A | PLC 3 |
High Volt Arc Track Rate | 23.0 °C | 2 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 2 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with Hot-Wire Ignition of 1.5 mm | ≥, UL 746A | PLC 2 |
Kriechstromfestigkeit | 23.0 °C | 4 V Show Supplier Material materials with Kriechstromfestigkeit of 4 V | UL 746A | (UL) {PLC} |
Technological properties
Property | ||
---|---|---|
Application areas | Meter Gas, Oil/Gas, Pharmaceutical Packaging & Drug Delivery, Wireless Communications, Wiring Devices, Data Transfer, Data Management, Document Handling, Aerospace, Circuit Protection, Auto Aftermarket, Energy Management, Enclosure/Housing/Cover, Enclosures, Electronic Components, Wire & cable | |
Availability | Europe,Asia,Americas | |
Processing methods | Melt Temperature: 370 to 410.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |