Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 227 MPa Show Supplier Material materials with Biegefestigkeit of 227 MPa | ASTM D 790 | brk, 2.6 mm/min, 100 mm span |
Biegemodul | 23.0 °C | 6.9 GPa Show Supplier Material materials with Biegemodul of 6.9 GPa | ASTM D 790 | 2.6 mm/min, 100 mm span |
Dehnung | 23.0 °C | 4 % Show Supplier Material materials with Dehnung of 4 % | ASTM D 638 | brk, Type I, 5 mm/min |
Elastizitätsmodul | 23.0 °C | 6.9 GPa Show Supplier Material materials with Elastizitätsmodul of 6.9 GPa | ASTM D 638 | 5 mm/min |
Zugfestigkeit | 23.0 °C | 131 MPa Show Supplier Material materials with Zugfestigkeit of 131 MPa | ASTM D 638 | brk, Type I, 5 mm/min |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Heat deflection temperature, 0.45 MPa | 210 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 210 °C | ASTM D 648 | 6.4 mm, unannealed | |||
Heat deflection temperature, 1.80 MPa | 210 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 210 °C | ASTM D 648 | 6.4 mm, unannealed | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2.52E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.52E-5 1/K | ASTM E 831 | -20°C to 150°C | ||
Relative temperature index, electrical | 170 °C Show Supplier Material materials with Relative temperature index, electrical of 170 °C | UL 746B | |||
Relative temperature index, mechanical impact | 170 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 170 °C | UL 746B | |||
Relative temperature index, mechanical strength | 170 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 170 °C | UL 746B | |||
Vicat-Erweichungstemperatur | 220 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 220 °C | ASTM D 1525 | Rate B/50 | |||
Wärmeformbeständigkeitstemperatur | 210 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 210 °C | ||||
Entflammbarkeit | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=100218986- - <br> UL Yellow Card Link 2: https://iq.ul.com/ul/cert.aspx?ULID=100218988- - <br> UL Recognized, 94-5VA Flame Class Rating: ≥1.9mm UL 94 <br> UL Recognized, 94V-0 Flame Class Rating: ≥0.38mm UL 94 <br> NBS Smoke Density, Flaming, Ds 4 min: 1.3- ASTM E 662 <br> UV-light, water exposure/immersion: F1- UL 746C <br> UL Yellow Card Link 3: https://iq.ul.com/ul/cert.aspx?ULID=236983- - |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Durchschlagfestigkeit | 23.0 °C | 26.3 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 26.3 kV/mm | ASTM D 149 | in oil, 1.6 mm |
High Amp Arc Ignition | 23.0 °C | 3 mm Show Supplier Material materials with High Amp Arc Ignition of 3 mm | ≥, UL 746A | PLC 4 |
High Volt Arc Track Rate | 23.0 °C | 2 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 2 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 3 mm Show Supplier Material materials with Hot-Wire Ignition of 3 mm | ≥, UL 746A | PLC 1 |
Kriechstromfestigkeit | 23.0 °C | 4 V Show Supplier Material materials with Kriechstromfestigkeit of 4 V | UL 746A | (UL) {PLC} |
Verlustfaktor | 23.0 °C | 4.9E-3 [-] Show Supplier Material materials with Verlustfaktor of 4.9E-3 [-] | ASTM D 150 | 2450 MHz |
Volume resistivity | 23.0 °C | 7.00E+16 Ω·cm Show Supplier Material materials with Volume resistivity of 7.00E+16 Ω·cm | ASTM D 257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 0.3 % Show Supplier Material materials with Schrumpfung of 0.3 % | SABIC method | on tensile bar |
Technological properties
Property | ||
---|---|---|
Application areas | Meter Water, Medical Device, Oil/Gas, Non-LED Lighting, Personal Computing, Pharmaceutical Packaging & Drug Delivery, Power Manangement, Wireless Communications, Weapon, Water Treatment/Filtration, Wiring Devices, Data Transfer, Displays, Circuit Protection, Aircraft Seating, Aerospace, Air Cabin Interiors, Fluid Delivery, Individual Equiptment, Enclosures, Enclosure/Housing/Cover, Electronics, Electronic Components, Wire & cable | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 150°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |