FLEX NORYL™ WCD801A resin is a flexible, non-reinforced, migration improved, extrudable blend of Polyphenylene Ether (PPE) + Thermoplastic Elastomer (TPE). This material contains non-halogenated flame retardant and performance capable of meeting UL VW-1 requirements, 80C end use temperature rating, and heat deformation performance as defined by UL 1581. FLEX NORYL WCD801A resin is intended for evaluation in wire insulation and cable jacket applications in dark colors. It has a Shore A Hardness reading of 80 and exhibits superior thermal stability, very low water absorption, good electric properties, and low specific gravity. Processing is typically conducted on standard extrusion equipment, and UL 1581 testing is conducted on 2.0mm wire with 0.12mm X 20 stranded copper conductor.

Diese Materialdaten wurden von Sabic zur Verfügung gestellt

Alle Daten beziehen sich auf Raumtemperatur soweit nicht anderweitig spezifiziert. SI Einheiten werden verwendt soweit nicht anderweitig spezifiziert.
Äquivalente Standards sind ähnlich zu einem oder mehreren Standards die der Anbieter angegeben hat. Manche äquivalente Standards können strikter sein oder außerhalb der Bedingungen des ursprünglichen Standards.

Ashby charts

Eigenschaften

Allgemein

PropertyTemperatureValueComment

Relative Dichte

23.0 °C

1.1 [-]

Show Supplier Material materials with Relative Dichte of 1.1 [-]

ASTM D 792 |

Sauerstoffindex

23.0 °C

26 %

Show Supplier Material materials with Sauerstoffindex of 26 %

Mechanisch

PropertyTemperatureValueComment

Biegemodul

23.0 °C

0.1 GPa

Show Supplier Material materials with Biegemodul of 0.1 GPa

ISO 178 | 12.5 mm/min

Dehnung

23.0 °C

119 %

Show Supplier Material materials with Dehnung of 119 %

ISO 527 | break, 50 mm/min

Härte, Shore A

23.0 °C

80 [-]

Show Supplier Material materials with Härte, Shore A of 80 [-]

ASTM D 2240 | 30S reading

Zugfestigkeit

23.0 °C

13 MPa

Show Supplier Material materials with Zugfestigkeit of 13 MPa

ISO 527 | break, 50 mm/min

Thermisch

PropertyValueComment

Brittleness temperature

-40 °C

Show Supplier Material materials with Brittleness temperature of -40 °C

<, ASTM D 746

Entflammbarkeit

Smoke Density on 0.5mm plaque, Flame, Ds, max: 142- ASTM E 662 <br> Smoke Density on 0.5mm plaque, Non-flame, Ds, max: 95- ASTM E 662 <br> Glow Wire Flammability Index 650°C, passes at: 3mm IEC 60695-2-12 <br> UL Recognized, 94V-0 Flame Class Rating: ≥4mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=536311- -

Elektrisch

PropertyTemperatureValueComment

Dielectric constant, 60Hz

23.0 °C

2.8 [-]

Show Supplier Material materials with Dielectric constant, 60Hz of 2.8 [-]

IEC 60250 | 50/60 Hz

Dielektrizitätskonstante, 1 MHz

23.0 °C

2.8 [-]

Show Supplier Material materials with Dielektrizitätskonstante, 1 MHz of 2.8 [-]

IEC 60250

Dissipation factor, 1MHz

23.0 °C

4E-3 [-]

Show Supplier Material materials with Dissipation factor, 1MHz of 4E-3 [-]

IEC 60250

Dissipation factor, 50Hz

23.0 °C

0.03 [-]

Show Supplier Material materials with Dissipation factor, 50Hz of 0.03 [-]

IEC 60250 | 50/60 Hz

Durchschlagfestigkeit

23.0 °C

23 kV/mm

Show Supplier Material materials with Durchschlagfestigkeit of 23 kV/mm

IEC 60243-1 | in oil, 2.0mm

Kriechstromfestigkeit

23.0 °C

600 V

Show Supplier Material materials with Kriechstromfestigkeit of 600 V

IEC 60112 |

Volume resistivity

23.0 °C

3.80E+15 Ω·cm

Show Supplier Material materials with Volume resistivity of 3.80E+15 Ω·cm

IEC 60093 |

Rheological Properties

PropertyValueComment

Schmelzmassenflussrate

11 g/10min

Show Supplier Material materials with Schmelzmassenflussrate of 11 g/10min

ASTM D 1238 | 250°C/5.0 kgf

Technological properties

Property
Application areas

Wireless Communications, Personal Computing, Enclosure/Housing/Cover, Heavy Vehicles, Freezer, Wire & cable

Availability

Americas

Processing methods

Melt Temperature: 220 to 250.0°C
Neck Temperature: 220 to 250.0°C
Head Zone Temperature: 220 to 250.0°C
Die Temperature: 220 to 250.0°C
Screw Speed: 15 to 85.0rpm
Screen Pack: 150 to 100.0-
Cross-head Temperature: 220 to 250.0°C
Water Bath Temperature: 15 to 60.0°C
Drying Time: 5 to 7.0hrs
Feed Zone Temperature: 180 to 220.0°C
Conductor Pre-heat Temperature: 25 to 120.0°C
Maximum Moisture Content: 0.02%
Drying Time (Cumulative): 12hrs
Middle Zone Temperatures: 220 to 250.0°C
Cooling Water Air Gap: 100 to 200.0mm
Drying Temperature: 75 to 85.0°C
Extruder Length/Diameter Ratio (L/D): 22:1 to 26:1-

Supplier Disclaimer

While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right.