Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 150 MPa Show Supplier Material materials with Biegefestigkeit of 150 MPa | ASTM D 790 | brk, 1.3 mm/min, 50 mm span |
Biegemodul | 23.0 °C | 8.3 GPa Show Supplier Material materials with Biegemodul of 8.3 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Dehnung | 23.0 °C | 6.4 % Show Supplier Material materials with Dehnung of 6.4 % | ASTM D 638 | brk, Type I, 5 mm/min |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 106 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 106 kJ/m² | ASTM D 256 | notched, 23°C |
Zugfestigkeit | 23.0 °C | 95 MPa Show Supplier Material materials with Zugfestigkeit of 95 MPa | ASTM D 638 | yld, Type I, 5 mm/min |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Heat deflection temperature, 0.45 MPa | 158 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 158 °C | ASTM D 648 | 3.2 mm, unannealed | |
Heat deflection temperature, 1.80 MPa | 146 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 146 °C | ASTM D 648 | 3.2mm, unannealed | |
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.08E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.08E-5 1/K | ASTM E 831 | -40°C to 40°C |
Vicat-Erweichungstemperatur | 163 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 163 °C | ASTM D 1525 | Rate B/50 | |
Wärmeformbeständigkeitstemperatur | 146 - 158 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 146 - 158 °C | ||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 6.3E-5 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 6.3E-5 1/K | ASTM E 831 | -40°C to 40°C |
Technological properties
Property | ||
---|---|---|
Application areas | Water Treatment/Filtration, Hot Water System | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Time (Cumulative): 8hrs | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |