Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.05 g/cm³ Show Supplier Material materials with Dichte of 1.05 g/cm³ | ISO 1183 |
Moisture absorption | 23.0 °C | 0.07 % Show Supplier Material materials with Moisture absorption of 0.07 % | ISO 62 | (23°C / 50% RH) |
Sauerstoffindex | 23.0 °C | 19 % Show Supplier Material materials with Sauerstoffindex of 19 % | |
Wasserabsorption | 23.0 °C | 0.2 % Show Supplier Material materials with Wasserabsorption of 0.2 % | ISO 62-1 | (23°C/saturated) |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 60 MPa Show Supplier Material materials with Biegefestigkeit of 60 MPa | ISO 178 | yield, 2 mm/min |
Biegemodul | 23.0 °C | 2 GPa Show Supplier Material materials with Biegemodul of 2 GPa | ISO 178 | 2 mm/min |
Dehnung | 23.0 °C | 30 % Show Supplier Material materials with Dehnung of 30 % | ISO 527 | break, 50 mm/min |
Elastizitätsmodul | 23.0 °C | 2.2 GPa Show Supplier Material materials with Elastizitätsmodul of 2.2 GPa | ISO 527 | 1 mm/min |
Hardness, Ball Indentation | 23.0 °C | 95 MPa Show Supplier Material materials with Hardness, Ball Indentation of 95 MPa | ISO 2039-1 | H358/30 |
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 5 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 5 kJ/m² | ISO 179/1eA | V-notch Edgew 80*10*4 sp=62mm, -30°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 11 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 11 kJ/m² | ISO 180/1A | 80*10*4, 23°C |
Zugfestigkeit | 23.0 °C | 45 MPa Show Supplier Material materials with Zugfestigkeit of 45 MPa | ISO 527 | yield, 50 mm/min |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Ball Pressure Test | nan | IEC 60695-10-2 | 75°C +/- 2°C | |||
Ball pressure temperature | 115 °C Show Supplier Material materials with Ball pressure temperature of 115 °C | IEC 60695-10-2 | approximate maximum | |||
Heat deflection temperature, 0.45 MPa | 105 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 105 °C | ISO 75/Be | Edgew 120*10*4 sp=100mm | |||
Heat deflection temperature, 1.80 MPa | 95 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 95 °C | ISO 75/Ae | Edgew 120*10*4 sp=100mm | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 7E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 7E-5 1/K | ISO 11359-2 | 23°C to 80°C | ||
Relative temperature index, electrical | 90 °C Show Supplier Material materials with Relative temperature index, electrical of 90 °C | UL 746B | |||
Relative temperature index, mechanical impact | 85 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 85 °C | UL 746B | |||
Relative temperature index, mechanical strength | 95 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 95 °C | UL 746B | |||
Vicat-Erweichungstemperatur | 115 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 115 °C | ISO 306 | Rate B/120 | |||
Wärmeformbeständigkeitstemperatur | 95 - 105 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 95 - 105 °C | ||||
Wärmeleitfähigkeit | 23.0 °C | 0.22 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 0.22 W/(m·K) | ISO 8302 | ||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 9E-5 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 9E-5 1/K | ISO 11359-2 | 23°C to 80°C | ||
Entflammbarkeit | Glow Wire Flammability Index 960°C, passes at: 3.2mm IEC 60695-2-12 <br> Glow Wire Flammability Index 960°C, passes at: 3.2mm IEC 60695-2-12 <br> UL Recognized, 94HB Flame Class Rating: ≥1.5mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=236761- - |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dielectric constant, 60Hz | 23.0 °C | 2.6 [-] Show Supplier Material materials with Dielectric constant, 60Hz of 2.6 [-] | IEC 60250 | 50/60 Hz |
Dielektrizitätskonstante, 1 MHz | 23.0 °C | 2.6 [-] Show Supplier Material materials with Dielektrizitätskonstante, 1 MHz of 2.6 [-] | IEC 60250 |
Dissipation factor, 1MHz | 23.0 °C | 1E-3 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 1E-3 [-] | IEC 60250 |
Dissipation factor, 50Hz | 23.0 °C | 4E-3 [-] Show Supplier Material materials with Dissipation factor, 50Hz of 4E-3 [-] | IEC 60250 | 50/60 Hz |
Durchschlagfestigkeit | 23.0 °C | 19 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 19 kV/mm | IEC 60243-1 | in oil, 3.2 mm, |
High Amp Arc Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with High Amp Arc Ignition of 1.5 mm | ≥, UL 746A | PLC 0 |
High Volt Arc Track Rate | 23.0 °C | 3 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 3 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with Hot-Wire Ignition of 1.5 mm | ≥, UL 746A | PLC 3 |
Kriechstromfestigkeit | 23.0 °C | 2 V Show Supplier Material materials with Kriechstromfestigkeit of 2 V | UL 746A | (UL) {PLC} |
Sheet resistivity, ROA | 23.0 °C | 1.00E+15 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+15 Ω | >, IEC 60093 |
Volume resistivity | 23.0 °C | 1.00E+15 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+15 Ω·cm | IEC 60093 | |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzvolumenflussrate | 15 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 15 cm³/10min | ISO 1133 | MVR at 280°C/3.8 kg | |
Schrumpfung | 23.0 °C | 0.5 % Show Supplier Material materials with Schrumpfung of 0.5 % | SABIC method | on tensile bar |
Technological properties
Property | ||
---|---|---|
Application areas | Personal Computing, Meter Water, Photovoltaic Components, Plumbing, Pharmaceutical Packaging & Drug Delivery, Refrigerator, Pump, Wheel Cover, Wiring Devices, Swimming Pool/Spa, Bottles, Cladding/Roof, Data Transfer, Circuit Protection, Electronic Components, Energy Management, Enclosures, Freezer, Heavy Vehicles, Lab Ware and Clinical Diagnostics | |
Availability | Europe | |
Processing methods | Nozzle Temperature: 260 to 280.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |