Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Wasserabsorption | 23.0 °C | 0.12 % Show Supplier Material materials with Wasserabsorption of 0.12 % | ISO 62-1 | (23°C/saturated) |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 115 MPa Show Supplier Material materials with Biegefestigkeit of 115 MPa | ISO 178 | yield, 2 mm/min |
Biegemodul | 23.0 °C | 4.2 GPa Show Supplier Material materials with Biegemodul of 4.2 GPa | ISO 178 |
Dehnung | 23.0 °C | 3 % Show Supplier Material materials with Dehnung of 3 % | ISO 527 | break |
Elastizitätsmodul | 23.0 °C | 3.9 GPa Show Supplier Material materials with Elastizitätsmodul of 3.9 GPa | ISO 527 | 1 mm/min |
Schlagzähigkeit, Izod ungekerbt | 23.0 °C | 30 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod ungekerbt of 30 kJ/m² | ISO 180/1U | unnotched 80*10*4, -30°C |
Zugfestigkeit | 23.0 °C | 60 MPa Show Supplier Material materials with Zugfestigkeit of 60 MPa | ISO 527 | break, 50 mm/min |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Heat deflection temperature, 0.45 MPa | 132 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 132 °C | ISO 75/Be | Edgew 120*10*4 sp=100mm | |||
Heat deflection temperature, 1.80 MPa | 124 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 124 °C | ISO 75/Ae | Edgew 120*10*4 sp=100mm | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 3.8E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 3.8E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Vicat-Erweichungstemperatur | 138 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 138 °C | ISO 306 | Rate B/50 | |||
Wärmeformbeständigkeitstemperatur | 124 - 132 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 124 - 132 °C | ||||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 7E-5 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 7E-5 1/K | ISO 11359-2 | 23°C to 80°C | ||
Entflammbarkeit | UL Recognized, 94HB Flame Class Rating: ≥1.5mm UL 94 <br> UV-light, water exposure/immersion: F1- UL 746C <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=228544- - <br> UL Yellow Card Link 2: https://iq.ul.com/ul/cert.aspx?ULID=237019- - |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Hot-Wire Ignition | 23.0 °C | 3 mm Show Supplier Material materials with Hot-Wire Ignition of 3 mm | ≥, UL 746A | PLC 0 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzvolumenflussrate | 8 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 8 cm³/10min | ISO 1133 | MVR at 280°C/5.0 kg | |
Schrumpfung | 23.0 °C | 0.2 % Show Supplier Material materials with Schrumpfung of 0.2 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Document Handling, Coffee Maker/Espresso Machine, Data Transfer, Air Conditioning, Air Filtration, Building Accessory, Circuit Protection, Enclosure/Housing/Cover, Energy Management, Enclosures, Electronic Components, Fixture Bath/Shower, Furnace/Heater, Hot Water System, Heavy Vehicles, Individual Equiptment, Lab Ware and Clinical Diagnostics, Swimming Pool/Spa, Water Treatment/Filtration, Wiring Devices, Wireless Communications, Medical Device, Meter Gas, Personal Computing, Recreational Vehicle, Pump, Pipe/Fitting, Plumbing, Security/Detection, Respiratory, Sanitary, Small Appliance, Irrigation | |
Availability | Europe,Asia,Americas | |
Processing methods | Screw Speed: 20 to 100.0rpm | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |