Allgemein
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 99 MPa Show Supplier Material materials with Biegefestigkeit of 99 MPa | ASTM D 790 | yld, 2.6 mm/min, 100 mm span |
Biegemodul | 23.0 °C | 2.3 GPa Show Supplier Material materials with Biegemodul of 2.3 GPa | ASTM D 790 | 2.6 mm/min, 100 mm span |
Dehnung | 23.0 °C | 30 % Show Supplier Material materials with Dehnung of 30 % | ASTM D 638 | brk, Type I, 50 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 288 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 288 J/m | ASTM D 256 |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 288 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 288 kJ/m² | ASTM D 256 | notched, 23°C |
Zugfestigkeit | 23.0 °C | 62 MPa Show Supplier Material materials with Zugfestigkeit of 62 MPa | ASTM D 638 | yld, Type I, 50 mm/min |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Heat deflection temperature, 0.45 MPa | 154 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 154 °C | ASTM D 648 | 6.4 mm, unannealed | |
Heat deflection temperature, 1.80 MPa | 146 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 146 °C | ASTM D 648 | 6.4 mm, unannealed | |
Koeffizient der thermischen Ausdehnung | 23.0 °C | 7.2E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 7.2E-5 1/K | ASTM E 831 | 0°C to 100°C |
Wärmeformbeständigkeitstemperatur | 146 - 154 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 146 - 154 °C |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 0.5 % Show Supplier Material materials with Schrumpfung of 0.5 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Gas/Electric Oven, Head Protection, Enclosures, Electronic Components, Data Transfer | |
Availability | Asia,Americas | |
Processing methods | Mold Temperature: 75 to 105.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |