Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 98 MPa Show Supplier Material materials with Biegefestigkeit of 98 MPa | ASTM D 790 | yld, 1.3 mm/min, 50 mm span |
Biegemodul | 23.0 °C | 2.4 GPa Show Supplier Material materials with Biegemodul of 2.4 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Dehnung | 23.0 °C | 53 % Show Supplier Material materials with Dehnung of 53 % | ASTM D 638 | brk, Type I, 50 mm/min |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 202 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 202 kJ/m² | ASTM D 256 | notched, 23°C |
Zugfestigkeit | 23.0 °C | 62 MPa Show Supplier Material materials with Zugfestigkeit of 62 MPa | ASTM D 638 | yld, Type I, 50 mm/min |
Thermisch
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 1.3 % Show Supplier Material materials with Schrumpfung of 1.3 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Electronic Components, Console, Cooking Range, Auto Electrical, Circuit Protection, Meter Gas | |
Availability | Europe,Asia,Americas | |
Processing methods | Shot to Cylinder Size: 30 to 50.0% | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |