Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.28 g/cm³ Show Supplier Material materials with Dichte of 1.28 g/cm³ | ISO 1183 |
Relative Dichte | 23.0 °C | 1.28 [-] Show Supplier Material materials with Relative Dichte of 1.28 [-] | ASTM D 792 | |
Sauerstoffindex | 23.0 °C | 46 % Show Supplier Material materials with Sauerstoffindex of 46 % |
Mechanisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Biegefestigkeit | 23.0 °C | 136 MPa Show Supplier Material materials with Biegefestigkeit of 136 MPa | ISO 178 | yield, 2 mm/min | ||
Biegemodul | 23.0 °C | 2.8 GPa Show Supplier Material materials with Biegemodul of 2.8 GPa | ISO 178 | 2 mm/min | ||
Dehnung | 23.0 °C | 7 % Show Supplier Material materials with Dehnung of 7 % | ISO 527 | yield, 50 mm/min | ||
Elastizitätsmodul | 23.0 °C | 2.9 GPa Show Supplier Material materials with Elastizitätsmodul of 2.9 GPa | ASTM D 638 | 5 mm/min | ||
Impact strength, Izod notched, ASTM | 23.0 °C | 70 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 70 J/m | ASTM D 256 | ||
Instrumented Impact Ductility | 23.0 °C | 100 % Show Supplier Material materials with Instrumented Impact Ductility of 100 % | ASTM D 3763 | 0°C | ||
Instrumented Impact, Total Energy | 23.0 °C | 93 J Show Supplier Material materials with Instrumented Impact, Total Energy of 93 J | ASTM D 3763 | 23°C | ||
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 11 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 11 kJ/m² | ISO 179/2C | 23°C | ||
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 6 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 6 kJ/m² | ISO 180/1A | notched 80*10*4, -30°C | ||
Zugfestigkeit | 23.0 °C | 97 MPa Show Supplier Material materials with Zugfestigkeit of 97 MPa | ISO 527 | yield, 50 mm/min | ||
Schlagzähigkeit, Izod ungekerbt | ISO 180/1U | unnotched 80*10*4, 23°C |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Heat deflection temperature, 0.45 MPa | 205 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 205 °C | ISO 75/Be | Edgew 120*10*4 sp=100mm | |||
Heat deflection temperature, 1.80 MPa | 190 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 190 °C | ISO 75/Ae | Edgew 120*10*4 sp=100mm | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 5E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 5E-5 1/K | ISO 11359-2 | 23°C to 150°C | ||
Relative temperature index, electrical | 105 °C Show Supplier Material materials with Relative temperature index, electrical of 105 °C | UL 746B | |||
Relative temperature index, mechanical impact | 105 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 105 °C | UL 746B | |||
Relative temperature index, mechanical strength | 105 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 105 °C | UL 746B | |||
Vicat-Erweichungstemperatur | 212 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 212 °C | ISO 306 | Rate B/50 | |||
Wärmeformbeständigkeitstemperatur | 190 - 205 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 190 - 205 °C | ||||
Wärmeleitfähigkeit | 23.0 °C | 0.19 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 0.19 W/(m·K) | ASTM C177 | ||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 5E-5 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 5E-5 1/K | ISO 11359-2 | 23°C to 150°C | ||
Entflammbarkeit | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=100737020- - <br> UL Recognized, 94V-0 Flame Class Rating: ≥0.75mm UL 94 <br> NBS Smoke Density, Flaming, Ds 4 min: 0.7- ASTM E 662 |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
High Amp Arc Ignition | 23.0 °C | 0.75 mm Show Supplier Material materials with High Amp Arc Ignition of 0.75 mm | ≥, UL 746A | PLC 1 |
Hot-Wire Ignition | 23.0 °C | 0.75 mm Show Supplier Material materials with Hot-Wire Ignition of 0.75 mm | ≥, UL 746A | PLC 2 |
Kriechstromfestigkeit | 23.0 °C | 4 V Show Supplier Material materials with Kriechstromfestigkeit of 4 V | UL 746A | (UL) {PLC} |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzmassenflussrate | 10 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 10 g/10min | ASTM D 1238 | 337°C/6.6 kgf | |
Schmelzvolumenflussrate | 14 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 14 cm³/10min | ISO 1133 | MVR at 360°C/5.0 kg | |
Schrumpfung | 23.0 °C | 0.5 % Show Supplier Material materials with Schrumpfung of 0.5 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Animal Testing, Electronic Components, Enclosure/Housing/Cover, Lab Ware and Clinical Diagnostics, Surgical Devices, Renal and Blood Handling, Pharmaceutical Packaging & Drug Delivery, Medical Device, Medical Facility Infrastructure, Surgical Tray, Wire & cable | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 150°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |