Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Relative Dichte | 23.0 °C | 1.27 [-] Show Supplier Material materials with Relative Dichte of 1.27 [-] | ASTM D 792 | |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 66 MPa Show Supplier Material materials with Biegefestigkeit of 66 MPa | Modified ASTM D790 | 5mm/min |
Dehnung | 23.0 °C | 1.6 % Show Supplier Material materials with Dehnung of 1.6 % | Modified ASTM D638 | 5mm/min |
Zugfestigkeit | 23.0 °C | 124 MPa Show Supplier Material materials with Zugfestigkeit of 124 MPa | Modified ASTM D638 | 5mm/min |
Thermisch
Technological properties
Property | ||
---|---|---|
Application areas | PANELS FOR AUTOMOBILES | |
Availability | Americas | |
Processing methods | Extruder L/D: 24- | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |