Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Wasserabsorption | 23.0 °C | 0.1 % Show Supplier Material materials with Wasserabsorption of 0.1 % | ASTM D 570 | (23°C/24hrs) |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 75 MPa Show Supplier Material materials with Biegefestigkeit of 75 MPa | ASTM D 790 | yld, 2.6 mm/min, 100 mm span |
Biegemodul | 23.0 °C | 2.2 GPa Show Supplier Material materials with Biegemodul of 2.2 GPa | ASTM D 790 | 2.6 mm/min, 100 mm span |
Dehnung | 23.0 °C | 30 % Show Supplier Material materials with Dehnung of 30 % | ASTM D 638 | brk, Type I, 50 mm/min |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 234 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 234 kJ/m² | ASTM D 256 | notched, 23°C |
Zugfestigkeit | 23.0 °C | 49 MPa Show Supplier Material materials with Zugfestigkeit of 49 MPa | ASTM D 638 | yld, Type I, 50 mm/min |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Heat deflection temperature, 0.45 MPa | 121 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 121 °C | ASTM D 648 | 6.4 mm, unannealed | |
Heat deflection temperature, 1.80 MPa | 112 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 112 °C | ASTM D 648 | 6.4 mm, unannealed | |
Koeffizient der thermischen Ausdehnung | 23.0 °C | 7.38E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 7.38E-5 1/K | ASTM E 831 | 0°C to 100°C |
Wärmeformbeständigkeitstemperatur | 112 - 121 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 112 - 121 °C |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 0.5 % Show Supplier Material materials with Schrumpfung of 0.5 % | SABIC method | on tensile bar |
Technological properties
Property | ||
---|---|---|
Application areas | Motorcycle, Refrigerator, Photovoltaic Components, Plumbing, Wearables, Wiring Devices, Auto Electrical, Audio, Auto Aftermarket, Data Management, Data Transfer, Document Handling, Drain Pan, Gas/Electric Oven, Heavy Vehicles, Hygiene/Personal Care, Food Transportation, Enclosures, Enclosure/Housing/Cover, Electronic Components | |
Availability | Europe,Asia,Americas | |
Processing methods | Nozzle Temperature: 275 to 305.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |