Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Relative Dichte | 23.0 °C | 1.03 [-] Show Supplier Material materials with Relative Dichte of 1.03 [-] | ASTM D 792 | |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegemodul | 23.0 °C | 0.1 GPa Show Supplier Material materials with Biegemodul of 0.1 GPa | ISO 178 | 12.5 mm/min |
Dehnung | 23.0 °C | 210 % Show Supplier Material materials with Dehnung of 210 % | ISO 527 | break, 50 mm/min |
Härte, Shore A | 23.0 °C | 89 [-] Show Supplier Material materials with Härte, Shore A of 89 [-] | ASTM D 2240 | 30S reading |
Zugfestigkeit | 23.0 °C | 18 MPa Show Supplier Material materials with Zugfestigkeit of 18 MPa | ISO 527 | break, 50 mm/min |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Glow Wire Ignition Temperature | 775 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 775 °C | IEC 60695-2-13 | 3.0 mm | |
Entflammbarkeit | Glow Wire Flammability Index 960°C, passes at: 3mm IEC 60695-2-12 <br> Glow Wire Flammability Index 960°C, passes at: 3mm IEC 60695-2-12 |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Kriechstromfestigkeit | 23.0 °C | 600 V Show Supplier Material materials with Kriechstromfestigkeit of 600 V | IEC 60112 | |
Volume resistivity | 23.0 °C | 4.70E+15 Ω·cm Show Supplier Material materials with Volume resistivity of 4.70E+15 Ω·cm | IEC 60093 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzmassenflussrate | 17 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 17 g/10min | ASTM D 1238 | 250°C/10.0 kgf |
Technological properties
Property | ||
---|---|---|
Application areas | Wireless Communications, Power Manangement, Heavy Vehicles, Wire & cable | |
Availability | Asia | |
Processing methods | Cooling Water Air Gap: 100 to 200.0mm | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |