Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.3 g/cm³ Show Supplier Material materials with Dichte of 1.3 g/cm³ | ISO 1183 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 80 MPa Show Supplier Material materials with Biegefestigkeit of 80 MPa | ASTM D 790 | yld, 1.3 mm/min, 50 mm span |
Biegemodul | 23.0 °C | 2 GPa Show Supplier Material materials with Biegemodul of 2 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Dehnung | 23.0 °C | 5 % Show Supplier Material materials with Dehnung of 5 % | ASTM D 638 | yld, Type I, 50 mm/min |
Elastizitätsmodul | 23.0 °C | 2 GPa Show Supplier Material materials with Elastizitätsmodul of 2 GPa | ASTM D 638 | 50 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 530 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 530 J/m | ASTM D 256 | notched, 23°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 530 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 530 kJ/m² | ASTM D 256 | notched, 23°C |
Zugfestigkeit | 23.0 °C | 46 MPa Show Supplier Material materials with Zugfestigkeit of 46 MPa | ASTM D 638 | brk, Type I, 50 mm/min |
Thermisch
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzvolumenflussrate | 15 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 15 cm³/10min | ISO 1133 | MVR at 300°C/1.2 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Displays | |
Availability | Asia | |
Processing methods | Maximum Moisture Content: 0.02% | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |