Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 241 MPa Show Supplier Material materials with Biegefestigkeit of 241 MPa | ASTM D 790 | yld, 2.6 mm/min, 100 mm span |
Biegemodul | 23.0 °C | 9.7 GPa Show Supplier Material materials with Biegemodul of 9.7 GPa | ASTM D 790 | 2.6 mm/min, 100 mm span |
Dehnung | 23.0 °C | 3 % Show Supplier Material materials with Dehnung of 3 % | ASTM D 638 | brk, Type I, 5 mm/min |
Elastizitätsmodul | 23.0 °C | 9 GPa Show Supplier Material materials with Elastizitätsmodul of 9 GPa | ASTM D 638 | 5 mm/min |
Zugfestigkeit | 23.0 °C | 155 MPa Show Supplier Material materials with Zugfestigkeit of 155 MPa | ASTM D 638 | brk, Type I, 5 mm/min |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 212 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 212 °C | ASTM D 648 | 6.4 mm, unannealed | |
Wärmeformbeständigkeitstemperatur | 212 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 212 °C | ||
Entflammbarkeit | NBS Smoke Density, Flaming, Dmax: 5- ASTM E 662 <br> NBS Smoke Density, Flaming, Ds 4 min: 5- ASTM E 662 <br> NBS Smoke Density, Flaming, Ds 1.5 min: 0- ASTM E 662 <br> OSU peak heat release rate (5 minute test): 40kW/m² FAR 25.853 <br> Vertical Burn a (60s) passes at: 0sec FAR 25.853 <br> Vertical Burn b (12s) passes at: 0sec FAR 25.853 <br> FAA Flammability, FAR 25.853 A/B: NATURAL- FAR 25.853 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 0.2 % Show Supplier Material materials with Schrumpfung of 0.2 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Enclosure/Housing/Cover, Air Cabin Interiors, Aircraft Seating, Aerospace | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Time (Cumulative): 24hrs | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |