Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Relative Dichte | 23.0 °C | 1.4 [-] Show Supplier Material materials with Relative Dichte of 1.4 [-] | ASTM D 792 | |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 206 MPa Show Supplier Material materials with Biegefestigkeit of 206 MPa | ASTM D 790 | yld, 2.6 mm/min, 100 mm span |
Biegemodul | 23.0 °C | 7.2 GPa Show Supplier Material materials with Biegemodul of 7.2 GPa | ASTM D 790 | 2.6 mm/min, 100 mm span |
Dehnung | 23.0 °C | 3 % Show Supplier Material materials with Dehnung of 3 % | ASTM D 638 | brk, Type I, 5 mm/min |
Elastizitätsmodul | 23.0 °C | 7 GPa Show Supplier Material materials with Elastizitätsmodul of 7 GPa | ASTM D 638 | 5 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 101 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 101 J/m | ASTM D 256 | notched, 23°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 101 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 101 kJ/m² | ASTM D 256 | notched, 23°C |
Zugfestigkeit | 23.0 °C | 151 MPa Show Supplier Material materials with Zugfestigkeit of 151 MPa | ASTM D 638 | brk, Type I, 5 mm/min |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 211 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 211 °C | ASTM D 648 | 6.4 mm, unannealed | |
Wärmeformbeständigkeitstemperatur | 211 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 211 °C | ||
Entflammbarkeit | NBS Smoke Density, Flaming, Ds 4 min: 5- ASTM E 662 <br> NBS Smoke Density, Flaming, Dmax: 5- ASTM E 662 <br> OSU peak heat release rate (5 minute test): 40kW/m² FAR 25.853 <br> Vertical Burn b (12s) passes at: 0sec FAR 25.853 <br> Vertical Burn a (60s) passes at: 0sec FAR 25.853 <br> NBS Smoke Density, Flaming, Ds 1.5 min: 0- ASTM E 662 <br> FAA Flammability, FAR 25.853 A/B: NATURAL- FAR 25.853 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzmassenflussrate | 5.7 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 5.7 g/10min | ASTM D 1238 | 337°C/6.6 kgf | |
Schrumpfung | 23.0 °C | 0.3 % Show Supplier Material materials with Schrumpfung of 0.3 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Aerospace, Aircraft Seating, Air Cabin Interiors, Electronic Components | |
Availability | Asia,Americas | |
Processing methods | Mold Temperature: 135 to 165.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |