Allgemein
Property | Value | Comment |
---|---|---|
Recycled Content | 82.1 % Show Supplier Material materials with Recycled Content of 82.1 % | Average recycled content |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 35 % Show Supplier Material materials with Dehnung of 35 % | min. |
Streckgrenze Rp 0,2 | 23.0 °C | 205 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 205 MPa | min. |
Zugfestigkeit | 23.0 °C | 510 - 690 MPa Show Supplier Material materials with Zugfestigkeit of 510 - 690 MPa |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Chrom | 16.5 % Show Supplier Material materials with Chrom of 16.5 % | ||
Eisen | Balance | ||
Kohlenstoff | 0.06 % Show Supplier Material materials with Kohlenstoff of 0.06 % | max. | |
Mangan | 1.3 % Show Supplier Material materials with Mangan of 1.3 % | ||
Nickel | 13 % Show Supplier Material materials with Nickel of 13 % | ||
Niobium | 0.7 % Show Supplier Material materials with Niobium of 0.7 % | ||
Phosphor | 0.02 % Show Supplier Material materials with Phosphor of 0.02 % | max. | |
Schwefel | 0.015 % Show Supplier Material materials with Schwefel of 0.015 % | max. | |
Silizium | 0.4 % Show Supplier Material materials with Silizium of 0.4 % |