Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 20.0 °C | 2.5 - 2.6 g/cm³ Show Supplier Material materials with Dichte of 2.5 - 2.6 g/cm³ | approx. |
Porosität | 0 % Show Supplier Material materials with Porosität of 0 % | approx., ISO 9385 |
Abmessung
Property | Value |
---|---|
Breite | 900 - 1100 mm Show Supplier Material materials with Breite of 900 - 1100 mm |
Dicke | 3 - 6 mm Show Supplier Material materials with Dicke of 3 - 6 mm |
Länge | 1600 - 1954 mm Show Supplier Material materials with Länge of 1600 - 1954 mm |
Dimensions | Flat cut-to-size panels and bent panels are also available. Formats of flat cut-to-size panels and bent panels on request. |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 20.0 °C | 100 - 165 MPa Show Supplier Material materials with Biegefestigkeit of 100 - 165 MPa | approx., DIN EN 1288, Part 5, R45 |
Elastizitätsmodul | 20.0 °C | 84 - 95 GPa Show Supplier Material materials with Elastizitätsmodul of 84 - 95 GPa | approx., ASTM C-1259 |
Härte, Knoop, HK2 | 20.0 °C | 570 - 600 [-] Show Supplier Material materials with Härte, Knoop, HK2 of 570 - 600 [-] | approx., ISO 9385 (HK 0.1/20) |
Poissonzahl | 20.0 °C | 0.25 - 0.26 [-] Show Supplier Material materials with Poissonzahl of 0.25 - 0.26 [-] | approx., ASTM C-1259 |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 50.0 °C | -8E-7 - 6E-7 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of -8E-7 - 6E-7 1/K | for 0-50°C, DIN ISO 51045-1, DIN ISO 7991 |
Max. Betriebstemperatur | 650 °C Show Supplier Material materials with Max. Betriebstemperatur of 650 °C | short heating (1h) hom. | |
Spezifische Wärmekapazität | 20.0 °C | 800 - 850 J/(kg·K) Show Supplier Material materials with Spezifische Wärmekapazität of 800 - 850 J/(kg·K) | for 20-100°C |
Wärmeleitfähigkeit | 90.0 °C | 1.5 - 1.7 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 1.5 - 1.7 W/(m·K) | DIN 51936, ASTM E 1461-01 |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dielektrizitätskonstante, 1 MHz | 25.0 °C | 6.5 - 7.8 [-] Show Supplier Material materials with Dielektrizitätskonstante, 1 MHz of 6.5 - 7.8 [-] | DIN 53483 |
Verlustfaktor | 25.0 °C | 0 - 0.02 [-] Show Supplier Material materials with Verlustfaktor of 0 - 0.02 [-] | 1MHz, DIN 53483 |
spezifischer Widerstand | 250.0 °C | 3.98E+6 - 1.58E+7 Ω·m Show Supplier Material materials with spezifischer Widerstand of 3.98E+6 - 1.58E+7 Ω·m | DIN 52326 |
350.0 °C | 158489 - 501187 Ω·m Show Supplier Material materials with spezifischer Widerstand of 158489 - 501187 Ω·m | DIN 52326 | |
Akustisch
Property | Temperature | Value | Comment |
---|---|---|---|
Schallgeschwindigkeit, longitudinal | 20.0 °C | 6300 - 6700 m/s Show Supplier Material materials with Schallgeschwindigkeit, longitudinal of 6300 - 6700 m/s | ASTM C-1259 |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 15 - 27 % Show Supplier Material materials with Aluminium of 15 - 27 % | Al₂O₃ (DIN EN 1748-2-1) |
Andere | 0 - 5 % Show Supplier Material materials with Andere of 0 - 5 % | (DIN EN 1748-2-1) |
Barium | 0 - 8 % Show Supplier Material materials with Barium of 0 - 8 % | BaO (DIN EN 1748-2-1) |
Kalium | 0 - 2 % Show Supplier Material materials with Kalium of 0 - 2 % | K₂O (DIN EN 1748-2-1) |
Kalzium | 0 - 8 % Show Supplier Material materials with Kalzium of 0 - 8 % | CaO (DIN EN 1748-2-1) |
Lithium | 0 - 5 % Show Supplier Material materials with Lithium of 0 - 5 % | Li₂O (DIN EN 1748-2-1) |
Magnesium | 0 - 8 % Show Supplier Material materials with Magnesium of 0 - 8 % | MgO (DIN EN 1748-2-1) |
Natrium | 0 - 2 % Show Supplier Material materials with Natrium of 0 - 2 % | Na₂O (DIN EN 1748-2-1) |
Silizium | 50 - 80 % Show Supplier Material materials with Silizium of 50 - 80 % | SiO₂ (DIN EN 1748-2-1) |
Titan | 0 - 5 % Show Supplier Material materials with Titan of 0 - 5 % | TiO₂ (DIN EN 1748-2-1) |
Zink | 0 - 5 % Show Supplier Material materials with Zink of 0 - 5 % | ZnO (DIN EN 1748-2-1) |
Zirkonium | 0 - 5 % Show Supplier Material materials with Zirkonium of 0 - 5 % | ZrO₂ (DIN EN 1748-2-1) |
Technological properties
Property | ||
---|---|---|
Application areas | The following applications are simply examples of areas where NEXTREMA® has already been put to use successfully: BBQ applications - NEXTREMA® provides perfect visibility into the grill and can be used to optimize diverse aspects of the barbecue experience; IR applications - NEXTREMA® transforms infrared heaters into eye-catching design features and protects heating elements stylishly; High temperature furnaces - Use NEXTREMA® to line ovens or apply support plates (e.g. in display manufacturing); Household appliances - NEXTREMA® revolutionizes designs for transparent heating elements and heat resistant thin film coatings; Functional design material - NEXTREMA® is a revolutionary material for innovative product and industry design. | |
Compliance | NEXTREMA® materials do not contain any harmful substances according to the European directive 2002/95/EC “Hazardous Substances in electrical and electronically Equipment” and fulfill the terms of RoHS without any concerns. | |
Corrosion properties | The chemical resistance of NEXTREMA® is more extensive than that of most other comparable materials: Acid resistance (DIN 12116) S 1-2; Alkaline resistance (ISO 695) A 1-2; Hydrolytic class (DIN ISO 719) HGB 1. | |
Processing methods | NEXTREMA® is practically process inert. Even under extreme conditions, the material will not have negative interactions with the process environment. There are no interfering process factors such as gas emissions from organic components. |