Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.76 g/cm³ Show Supplier Material materials with Dichte of 1.76 g/cm³ | ISO 1183 |
Wasserabsorption | 23.0 °C | 0.02 % Show Supplier Material materials with Wasserabsorption of 0.02 % | ISO 62 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 285 MPa Show Supplier Material materials with Biegefestigkeit of 285 MPa | ISO 178 |
Biegemodul | 23.0 °C | 18 GPa Show Supplier Material materials with Biegemodul of 18 GPa | ISO 178 |
Dehnung | 23.0 °C | 1.7 % Show Supplier Material materials with Dehnung of 1.7 % | ISO 527 |
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 9 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 9 kJ/m² | ISO 179 |
Zugfestigkeit | 23.0 °C | 185 MPa Show Supplier Material materials with Zugfestigkeit of 185 MPa | ISO 527 |
Thermisch
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dielektrizitätskonstante | 23.0 °C | 4.5 [-] Show Supplier Material materials with Dielektrizitätskonstante of 4.5 [-] | IEC 60250 |
Durchschlagfestigkeit | 23.0 °C | 16 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 16 kV/mm | IEC 60243 |
Kriechstromfestigkeit | 23.0 °C | 155 V Show Supplier Material materials with Kriechstromfestigkeit of 155 V | IEC 60112 |
Verlustfaktor | 23.0 °C | 2E-3 [-] Show Supplier Material materials with Verlustfaktor of 2E-3 [-] | IEC 60250 |
Volume resistivity | 23.0 °C | 2.00E+15 Ω·cm Show Supplier Material materials with Volume resistivity of 2.00E+15 Ω·cm | IEC 60093 |
Technological properties
Property | ||
---|---|---|
Application areas | Can be used in auto parts such as thermostat housing,water pump cap,regulator,and other industrial fileds. | |
Fillers | 50% Glass Fiber | |
Processing methods | Injection Moulding / Test Specimen Production: Drying: 150°C & 3 hours - Injection Pressure: 30-100 MPa - Injection Molding Melt Temperature: 290-330°C - Injection Molding Mold Temperature: 120-160°C - Limit in-cylinder Retention Time: 300°C/60min or 320°C/30min |