Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.45 g/cm³ Show Supplier Material materials with Dichte of 1.45 g/cm³ | ISO 1183 |
Wasserabsorption | 23.0 °C | 0.04 % Show Supplier Material materials with Wasserabsorption of 0.04 % | ISO 62 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 340 MPa Show Supplier Material materials with Biegefestigkeit of 340 MPa | ISO 178 |
Biegemodul | 23.0 °C | 30 GPa Show Supplier Material materials with Biegemodul of 30 GPa | ISO 178 |
Dehnung | 23.0 °C | 0.7 % Show Supplier Material materials with Dehnung of 0.7 % | ISO 527 |
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 14 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 14 kJ/m² | ISO 179 |
Zugfestigkeit | 23.0 °C | 200 MPa Show Supplier Material materials with Zugfestigkeit of 200 MPa | ISO 527 |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 280 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 280 °C | ISO 75 | |
Entflammbarkeit | V-0, UL-94 |
Technological properties
Property | ||
---|---|---|
Application areas | Can be used in vacuum pump impeller,oilfield accessories and other components | |
Fillers | 30% Long Carbon Fiber | |
Processing methods | Injection Moulding / Test Specimen Production: Drying: 150°C & 3 hours - Injection Pressure: 30-100 MPa - Injection Molding Melt Temperature: 290-330°C - Injection Molding Mold Temperature: 120-160°C - Limit in-cylinder Retention Time: 300°C/60min or 320°C/30min |