Allgemein
Property | Value |
---|---|
Dichte | 1.3 - 1.8 g/cm³ Show Supplier Material materials with Dichte of 1.3 - 1.8 g/cm³ |
Abmessung
Thermisch
Property | Value | Comment |
---|---|---|
Wärmeleitfähigkeit | 5.0 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 5.0 W/(m·K) | through plane, Transverse |
300.0 - 500.0 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 300.0 - 500.0 W/(m·K) | in plane |
Elektrisch
Property | Value | Comment |
---|---|---|
spezifischer Widerstand | 5e-06 Ω·m Show Supplier Material materials with spezifischer Widerstand of 5e-06 Ω·m | in plane |
0.0007999999999999999 Ω·m Show Supplier Material materials with spezifischer Widerstand of 0.0007999999999999999 Ω·m | through plane, Transverse |
Technological properties
Property | ||
---|---|---|
Application areas | Many heat dissipation applications benefit from the outstanding properties of our SIGRATHERM high density (HD) foils. |