Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.25 g/cm³ Show Supplier Material materials with Dichte of 1.25 g/cm³ | ISO1183 |
Wasserabsorption | 23.0 °C | 1.25 % Show Supplier Material materials with Wasserabsorption of 1.25 % |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 175 MPa Show Supplier Material materials with Biegefestigkeit of 175 MPa | ISO178 |
Biegemodul | 23.0 °C | 4.5 GPa Show Supplier Material materials with Biegemodul of 4.5 GPa | ISO178 |
Dehnung | 23.0 °C | 6.5 % Show Supplier Material materials with Dehnung of 6.5 % | ISO527 |
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 12 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 12 kJ/m² | ISO179 |
Schlagzähigkeit, Charpy ungekerbt | 23.0 °C | 80 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 80 kJ/m² | ISO179 |
Zugfestigkeit | 23.0 °C | 125 MPa Show Supplier Material materials with Zugfestigkeit of 125 MPa | ISO527 |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 210 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 210 °C | ISO 75/A | |
Schmelzpunkt | 225 - 230 °C Show Supplier Material materials with Schmelzpunkt of 225 - 230 °C | ISO3146 | |
Entflammbarkeit | HB UL94 |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Durchschlagfestigkeit | 23.0 °C | 20 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 20 kV/mm | GB/T 1408 |
Volume resistivity | 23.0 °C | 1.00E+17 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+17 Ω·cm | GB/T1410 |
Technological properties
Property | ||
---|---|---|
Application areas | Automotive industry, mechanical shields, blades, gears, power tools, etc. | |
Fillers | 18% Glass Fiber |