Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.39 g/cm³ Show Supplier Material materials with Dichte of 1.39 g/cm³ | ISO1183 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 275 MPa Show Supplier Material materials with Biegefestigkeit of 275 MPa | ISO178 |
Biegemodul | 23.0 °C | 8.5 GPa Show Supplier Material materials with Biegemodul of 8.5 GPa | ISO178 |
Dehnung | 23.0 °C | 6 % Show Supplier Material materials with Dehnung of 6 % | ISO527 |
Hardness, Rockwell L | 23.0 °C | 106 [-] Show Supplier Material materials with Hardness, Rockwell L of 106 [-] | ISO 2039 |
Hardness, Rockwell R | 23.0 °C | 115 [-] Show Supplier Material materials with Hardness, Rockwell R of 115 [-] | ISO 2039 |
Härte, Rockwell M | 23.0 °C | 95 [-] Show Supplier Material materials with Härte, Rockwell M of 95 [-] | ISO 2039 |
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 12 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 12 kJ/m² | ISO179 |
Schlagzähigkeit, Charpy ungekerbt | 23.0 °C | 70 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 70 kJ/m² | ISO179 |
Zugfestigkeit | 23.0 °C | 185 MPa Show Supplier Material materials with Zugfestigkeit of 185 MPa | ISO527 |
Thermisch
Property | Value | Comment |
---|---|---|
Heat deflection temperature, 1.80 MPa | 254 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 254 °C | ISO 75/A |
Schmelzpunkt | 265 - 270 °C Show Supplier Material materials with Schmelzpunkt of 265 - 270 °C | ISO3146 |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Volume resistivity | 23.0 °C | 1.00E+17 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+17 Ω·cm | GB/T1410 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzmassenflussrate | 23 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 23 g/10min | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | Automotive industry, machinery shields, military products, building materials, etc. | |
Fillers | 33% Glass Fiber |