Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.09 g/cm³ Show Supplier Material materials with Dichte of 1.09 g/cm³ | ISO1183 |
Mechanisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Biegefestigkeit | 23.0 °C | 75 MPa Show Supplier Material materials with Biegefestigkeit of 75 MPa | ISO178 | ||
Biegemodul | 23.0 °C | 1.8 GPa Show Supplier Material materials with Biegemodul of 1.8 GPa | ISO178 | ||
Dehnung | 23.0 °C | 35 % Show Supplier Material materials with Dehnung of 35 % | ISO527 | ||
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 45 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 45 kJ/m² | ISO179 | ||
Zugfestigkeit | 23.0 °C | 55 MPa Show Supplier Material materials with Zugfestigkeit of 55 MPa | ISO527 | ||
Schlagzähigkeit, Charpy ungekerbt | No Break, ISO179 |
Thermisch
Property | Value | Comment |
---|---|---|
Schmelzpunkt | 260 - 265 °C Show Supplier Material materials with Schmelzpunkt of 260 - 265 °C | ISO3146 |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Volume resistivity | 23.0 °C | 1.00E+17 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+17 Ω·cm | GB/T1410 |
Technological properties
Property | ||
---|---|---|
Application areas | Automotive industry, railway parts, garden machinery, sports equipment, etc. |