Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.12 g/cm³ Show Supplier Material materials with Dichte of 1.12 g/cm³ | ISO1183 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 125 MPa Show Supplier Material materials with Biegefestigkeit of 125 MPa | ISO178 |
Biegemodul | 23.0 °C | 6 GPa Show Supplier Material materials with Biegemodul of 6 GPa | ISO178 |
Dehnung | 23.0 °C | 5 % Show Supplier Material materials with Dehnung of 5 % | ISO527 |
Schlagzähigkeit, Charpy ungekerbt | 23.0 °C | 45 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 45 kJ/m² | ISO179 |
Zugfestigkeit | 23.0 °C | 80 MPa Show Supplier Material materials with Zugfestigkeit of 80 MPa | ISO527 |
Technological properties
Property | ||
---|---|---|
Application areas | Automotive industry, consumer goods, etc. | |
Fillers | 30% Glass Fiber |