Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.22 g/cm³ Show Supplier Material materials with Dichte of 1.22 g/cm³ | ISO1183 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 125 MPa Show Supplier Material materials with Biegefestigkeit of 125 MPa | ISO178 |
Biegemodul | 23.0 °C | 7.2 GPa Show Supplier Material materials with Biegemodul of 7.2 GPa | ISO178 |
Schlagzähigkeit, Charpy ungekerbt | 23.0 °C | 40 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 40 kJ/m² | ISO179 |
Zugfestigkeit | 23.0 °C | 85 MPa Show Supplier Material materials with Zugfestigkeit of 85 MPa | ISO527 |
Technological properties
Property | ||
---|---|---|
Application areas | Automotive industry, consumer goods, etc. | |
Fillers | 40% Glass Fiber |