Allgemein
Property | Value | Comment |
---|---|---|
Partikelgröße D50 | 0.8 - 1 μm Show Supplier Material materials with Partikelgröße D50 of 0.8 - 1 μm | |
Spezifische Oberfläche | 10 - 15 m²/g Show Supplier Material materials with Spezifische Oberfläche of 10 - 15 m²/g | measured with the BET-method |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 0.01 % Show Supplier Material materials with Aluminium of 0.01 % | Al₂O₃ |
Chlor | 0.03 - 0.08 % Show Supplier Material materials with Chlor of 0.03 - 0.08 % | |
Eisen | 3E-3 % Show Supplier Material materials with Eisen of 3E-3 % | Fe₂O₃ |
Natrium | 0.01 % Show Supplier Material materials with Natrium of 0.01 % | Na₂O |
Silizium | 0.02 % Show Supplier Material materials with Silizium of 0.02 % | SiO₂ |
Titan | 0.01 % Show Supplier Material materials with Titan of 0.01 % | TiO₂ |
Yttrium | 8.37 - 8.77 % Show Supplier Material materials with Yttrium of 8.37 - 8.77 % | Y₂O₃ |
Zirkonium | 91.19 - 91.59 % Show Supplier Material materials with Zirkonium of 91.19 - 91.59 % | ZrO₂ |
Technological properties
Property | ||
---|---|---|
Application areas | YSZ powder is suitable for production of different structure ceramics,electronic ceramics,biological ceramics,advanced refractory,optical communication device,man-made jewelry,sensor ,solid fuel battery,grinding and polish trade and so on. Structural Ceramics: since nano ZrO2 ceramics with high toughness, high flexural strength and high wear resistance, excellent thermal insulation properties, thermal expansion coefficient close to steel, etc., nano ZrO2 powder is widely used in the field of structural ceramics. |