Abmessung
Property | Value |
---|---|
Breite | 1000 - 2000 mm Show Supplier Material materials with Breite of 1000 - 2000 mm |
Dicke | 0.5 - 50 mm Show Supplier Material materials with Dicke of 0.5 - 50 mm |
Länge | 2000 - 6000 mm Show Supplier Material materials with Länge of 2000 - 6000 mm |
Mechanisch
Property | Temperature | Value |
---|---|---|
Charpy impact energy, V-notch | -195.0 °C | 60 J Show Supplier Material materials with Charpy impact energy, V-notch of 60 J |
Dehnung | 23.0 °C | 40 % Show Supplier Material materials with Dehnung of 40 % |
Härte, Brinell | 23.0 °C | 215 [-] Show Supplier Material materials with Härte, Brinell of 215 [-] |
Streckgrenze Rp 0,2 | 23.0 °C | 200 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 200 MPa |
Zugfestigkeit | 23.0 °C | 515 - 700 MPa Show Supplier Material materials with Zugfestigkeit of 515 - 700 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 17.5 - 19.5 % Show Supplier Material materials with Chrom of 17.5 - 19.5 % |
Eisen | Balance |
Kohlenstoff | 0.07 % Show Supplier Material materials with Kohlenstoff of 0.07 % |
Mangan | 2 % Show Supplier Material materials with Mangan of 2 % |
Nickel | 8 - 10.5 % Show Supplier Material materials with Nickel of 8 - 10.5 % |
Phosphor | 0.05 % Show Supplier Material materials with Phosphor of 0.05 % |
Schwefel | 0.03 % Show Supplier Material materials with Schwefel of 0.03 % |
Silizium | 1 % Show Supplier Material materials with Silizium of 1 % |
Technological properties
Property | ||
---|---|---|
Application areas | Material AISI 304/ 304L is used in the chemical industry, food industry, pulp and paper industry and nuclear industry. | |
Corrosion properties | The grade is a versatile, general purpose stainless steel with good resistance to atmospheric corrosion, to many organic and inorganic chemicals, to oxidizing acids like nitric acid, caustic solutions at moderate temperatures and to food and beverages | |
Heat Treatment | Solution annealed and quenched in air or water. | |
Welding | Very good |