Allgemein
Property | Value |
---|---|
Partikelgröße D10 | 66 μm Show Supplier Material materials with Partikelgröße D10 of 66 μm |
Partikelgröße D50 | 107 μm Show Supplier Material materials with Partikelgröße D50 of 107 μm |
Partikelgröße D90 | 195 μm Show Supplier Material materials with Partikelgröße D90 of 195 μm |
Schüttdichte | 2.66 g/cm³ Show Supplier Material materials with Schüttdichte of 2.66 g/cm³ |
Rheological Properties
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminium | 5.5 - 6.5 % Show Supplier Material materials with Aluminium of 5.5 - 6.5 % | ||
Andere | 0.4 % Show Supplier Material materials with Andere of 0.4 % | Total Maximum | |
Eisen | 0.25 % Show Supplier Material materials with Eisen of 0.25 % | ||
Kohlenstoff | 0.08 % Show Supplier Material materials with Kohlenstoff of 0.08 % | Maximum | |
Sauerstoff | 0.13 % Show Supplier Material materials with Sauerstoff of 0.13 % | ||
Stickstoff | 0.03 % Show Supplier Material materials with Stickstoff of 0.03 % | ||
Titan | Balance | ||
Vanadium | 3.5 - 4.5 % Show Supplier Material materials with Vanadium of 3.5 - 4.5 % | ||
Wasserstoff | 0.0125 % Show Supplier Material materials with Wasserstoff of 0.0125 % |
Technological properties
Property | ||
---|---|---|
Application areas | Additive manufacturing, Metal Injection Molding, Thermal Spray, Biomedical, Aerospace |