Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 7.85 g/cm³ Show Supplier Material materials with Dichte of 7.85 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 19 % Show Supplier Material materials with Dehnung of 19 % |
Streckgrenze | 23.0 °C | 355 MPa Show Supplier Material materials with Streckgrenze of 355 MPa |
Zugfestigkeit | 23.0 °C | 490 - 620 MPa Show Supplier Material materials with Zugfestigkeit of 490 - 620 MPa |
Chemical properties
Property | Value |
---|---|
Kohlenstoff | 0.18 % Show Supplier Material materials with Kohlenstoff of 0.18 % |
Mangan | 0.9 - 1.6 % Show Supplier Material materials with Mangan of 0.9 - 1.6 % |
Phosphor | 0.04 % Show Supplier Material materials with Phosphor of 0.04 % |
Schwefel | 0.035 % Show Supplier Material materials with Schwefel of 0.035 % |
Silizium | 0.1 - 0.5 % Show Supplier Material materials with Silizium of 0.1 - 0.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | Shipbuilding, Offshore Building |