Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 7.98 g/cm³ Show Supplier Material materials with Dichte of 7.98 g/cm³ |
Mechanisch
Chemical properties
Property | Value |
---|---|
Chrom | 24 - 26 % Show Supplier Material materials with Chrom of 24 - 26 % |
Kohlenstoff | 0.08 % Show Supplier Material materials with Kohlenstoff of 0.08 % |
Mangan | 2 % Show Supplier Material materials with Mangan of 2 % |
Nickel | 19 - 22 % Show Supplier Material materials with Nickel of 19 - 22 % |
Phosphor | 0.05 % Show Supplier Material materials with Phosphor of 0.05 % |
Schwefel | 0.03 % Show Supplier Material materials with Schwefel of 0.03 % |
Silizium | 1.5 % Show Supplier Material materials with Silizium of 1.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | Pressure Vessel& Anti-Corrosion Building |