Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 6.8 g/cm³ Show Supplier Material materials with Dichte of 6.8 g/cm³ | |
Partikelgröße D50 | 2 μm Show Supplier Material materials with Partikelgröße D50 of 2 μm | |
Partikelgröße D90 | 5 μm Show Supplier Material materials with Partikelgröße D90 of 5 μm | |
Sieve residue 45μm | 1.0 % Show Supplier Material materials with Sieve residue 45μm of 1.0 % | max. |
Volatile share | 0.1 % Show Supplier Material materials with Volatile share of 0.1 % | at 105°C |
Mechanisch
Property | Value |
---|---|
Härte, Mohs | 2 [-] Show Supplier Material materials with Härte, Mohs of 2 [-] |
Thermisch
Property | Value | Comment |
---|---|---|
Max. Betriebstemperatur | 400.0 °C Show Supplier Material materials with Max. Betriebstemperatur of 400.0 °C | |
Oxidierungsschwelle | 400.0 °C Show Supplier Material materials with Oxidierungsschwelle of 400.0 °C | min. |
Schmelzpunkt | 685.0 °C Show Supplier Material materials with Schmelzpunkt of 685.0 °C | |
Spezifische Wärmekapazität | 280.0 J/(kg·K) Show Supplier Material materials with Spezifische Wärmekapazität of 280.0 J/(kg·K) | |
Temperaturleitfähigkeit | 0.252 mm²/s Show Supplier Material materials with Temperaturleitfähigkeit of 0.252 mm²/s | |
Wärmeleitfähigkeit | 0.379 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 0.379 W/(m·K) |
Elektrisch
Chemical properties
Property | Value |
---|---|
Bismut | 80.0 % Show Supplier Material materials with Bismut of 80.0 % |
Schwefel | 17.0 - 20.0 % Show Supplier Material materials with Schwefel of 17.0 - 20.0 % |
Technological properties
Property | ||
---|---|---|
Application areas | Tribotecc® BIS 84 bismuth sulfide is characterised by a particularly low melting point and low metal hardness. Combined with the ability to form protective layers of different contact surfaces over a wide range of temperatures and pressures, and excellent wear, friction and alloying properties as an additive, this product is ideal for a wide range of applications: E.g. in the plastics-, automotive-, machinery- and construction industries as well as in ceramics and medical technology. | |
Color | Grey |