Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 3.1 g/cm³ Show Supplier Material materials with Dichte of 3.1 g/cm³ | |
Partikelgröße D50 | 8 μm Show Supplier Material materials with Partikelgröße D50 of 8 μm | |
Partikelgröße D90 | 24 μm Show Supplier Material materials with Partikelgröße D90 of 24 μm | |
Poured density | 0.75 g/cm² Show Supplier Material materials with Poured density of 0.75 g/cm² | |
1 g/cm² Show Supplier Material materials with Poured density of 1 g/cm² | ||
Sieve residue 45μm | 4.0 % Show Supplier Material materials with Sieve residue 45μm of 4.0 % | max. |
Tamped Volume | 60 ml/100g Show Supplier Material materials with Tamped Volume of 60 ml/100g | |
90 ml/100g Show Supplier Material materials with Tamped Volume of 90 ml/100g | ||
Volatile share | 0.1 % Show Supplier Material materials with Volatile share of 0.1 % | at 105°C |
Thermisch
Chemical properties
Technological properties
Property | ||
---|---|---|
Application areas | Tribotecc® SLS 22 is characterized by its excellent tribological characteristics. Combined with the ability to form stable layers of different contact surfaces over a wide range of temperatures and pressures, and excellent wear and friction properties, this product is ideal for a wide range of applications: E.g. as an additive in lubricants in the form of greases, pastes and oils; in the plastic industry; powder metallurgy; as coatings in general; | |
Color | Bright |