Allgemein
Thermisch
Property | Value |
---|---|
Max. Betriebstemperatur | 400.0 °C Show Supplier Material materials with Max. Betriebstemperatur of 400.0 °C |
Chemical properties
Property | Value |
---|---|
Zinn | 64.0 % Show Supplier Material materials with Zinn of 64.0 % |
Technological properties
Property | ||
---|---|---|
Application areas | Friction: High tech friction materials to improve pad and disc wear; NVH characteristics; Lubricants: Greases, pastes and oils to reduce coefficient of friction and wear and improve emergency running properties; Plastics: Highly engineered thermoplastics to improve wear and durability; Other applications: Coatings, powder metallurgy, carbon brushes | |
Color | Mosaic-gold |