Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 2.8 g/cm³ Show Supplier Material materials with Dichte of 2.8 g/cm³ | |
Partikelgröße D50 | 2 - 5 μm Show Supplier Material materials with Partikelgröße D50 of 2 - 5 μm | ||
Partikelgröße D90 | 5 - 8 μm Show Supplier Material materials with Partikelgröße D90 of 5 - 8 μm | ||
Poured density | 23.0 °C | 0.45 - 0.75 g/cm² Show Supplier Material materials with Poured density of 0.45 - 0.75 g/cm² | |
Sieve residue 45μm | 2 % Show Supplier Material materials with Sieve residue 45μm of 2 % | max. | |
Tamped Volume | 80 - 120 ml/100g Show Supplier Material materials with Tamped Volume of 80 - 120 ml/100g | ||
Volatile share | 0.5 % Show Supplier Material materials with Volatile share of 0.5 % | at 105°C |
Thermisch
Property | Value | Comment |
---|---|---|
Oxidierungsschwelle | 520 °C Show Supplier Material materials with Oxidierungsschwelle of 520 °C | min. |
Chemical properties
Property | Value |
---|---|
Zink | 18 % Show Supplier Material materials with Zink of 18 % |
Technological properties
Property | ||
---|---|---|
Application areas | Tribotecc® SLS White F6 is characterized by its excellent tribological characteristics. Combined with the ability to form stable layers of different contact surfaces over a wide range of temperatures and pressures, and excellent wear and friction properties, this product is ideal for a wide range of applications: E.g. as an additive in lubricants in the form of greases, pastes and oils; in the plastic industry; powder metallurgy; as coatings and in metal forming in general; food industry | |
Color | White |