Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 4.3 - 4.9 g/cm³ Show Supplier Material materials with Dichte of 4.3 - 4.9 g/cm³ | |
Partikelgröße D50 | 7 - 30 μm Show Supplier Material materials with Partikelgröße D50 of 7 - 30 μm | ||
Partikelgröße D90 | 15 - 40 μm Show Supplier Material materials with Partikelgröße D90 of 15 - 40 μm | ||
Volatile share | 0.5 % Show Supplier Material materials with Volatile share of 0.5 % | at 105°C |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Max. Betriebstemperatur | 400 °C Show Supplier Material materials with Max. Betriebstemperatur of 400 °C | ||
Oxidierungsschwelle | 400 °C Show Supplier Material materials with Oxidierungsschwelle of 400 °C | min. | |
Schmelzpunkt | 1100 °C Show Supplier Material materials with Schmelzpunkt of 1100 °C | ||
Spezifische Wärmekapazität | 23.0 °C | 324 J/(kg·K) Show Supplier Material materials with Spezifische Wärmekapazität of 324 J/(kg·K) | |
Temperaturleitfähigkeit | 23.0 °C | 1.34 mm²/s Show Supplier Material materials with Temperaturleitfähigkeit of 1.34 mm²/s | |
Wärmeleitfähigkeit | 23.0 °C | 1.13 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 1.13 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 140000 S/m Show Supplier Material materials with Elektrische Leitfähigkeit of 140000 S/m |
spezifischer Widerstand | 23.0 °C | 7E-6 Ω·m Show Supplier Material materials with spezifischer Widerstand of 7E-6 Ω·m |
Technological properties
Property | ||
---|---|---|
Application areas | Tribotecc® CB 500 Copper-(II)-sulfide is characterised by its excellent absorbens and catalytical properties. Combined with the ability to form stable layers of different contact surfaces over a wide range of temperatures and pressures and excellent wear and friction properties as an additive, this product is ideal for a wide range of applications: E.g. in the areas of: | |
Color | Blue, Black |