Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.28 g/cm³ Show Material materials with Dichte of 7.28 g/cm³ | Typical for Pure/Low Alloyed Tin |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2.1E-5 - 2.9E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.1E-5 - 2.9E-5 1/K | Typical for Pure/Low Alloyed Tin |
Schmelzpunkt | 232 °C Show Material materials with Schmelzpunkt of 232 °C | Typical for Pure/Low Alloyed Tin | |
Spezifische Wärmekapazität | 23.0 °C | 205 - 238 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 205 - 238 J/(kg·K) | Typical for Pure/Low Alloyed Tin |
Wärmeleitfähigkeit | 23.0 °C | 52 - 74 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 52 - 74 W/(m·K) | Typical for Pure/Low Alloyed Tin |
Chemical properties
Property | Value |
---|---|
Zinn | 99 % Show Material materials with Zinn of 99 % |