Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzpunkt | 215 - 350 °C Show Material materials with Schmelzpunkt of 215 - 350 °C | Typical for Tin Antimony | |
Wärmeleitfähigkeit | 23.0 °C | 40 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 40 W/(m·K) | Typical for Tin Antimony |
Chemical properties
Property | Value |
---|---|
Antimon | 6.5 - 7.5 % Show Material materials with Antimon of 6.5 - 7.5 % |
Bismut | 0.5 % Show Material materials with Bismut of 0.5 % |
Blei | 0.25 % Show Material materials with Blei of 0.25 % |
Cadmium | 0.05 % Show Material materials with Cadmium of 0.05 % |
Kupfer | 0.05 % Show Material materials with Kupfer of 0.05 % |
Silber | 0.05 % Show Material materials with Silber of 0.05 % |
Zinn | 92.5 % Show Material materials with Zinn of 92.5 % |