Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 10.2 g/cm³ Show Material materials with Dichte of 10.2 g/cm³ | Typical for Molybdenum |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 20.0 °C | 10 - 20 % Show Material materials with Dehnung A50 of 10 - 20 % | |
Elastizitätsmodul | 23.0 °C | 324 GPa Show Material materials with Elastizitätsmodul of 324 GPa | Typical for Molybdenum |
Härte, Vickers, 10 | 20.0 °C | 215 [-] Show Material materials with Härte, Vickers, 10 of 215 [-] | |
Poissonzahl | 23.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Molybdenum |
Schubmodule | 23.0 °C | 125 GPa Show Material materials with Schubmodule of 125 GPa | Typical for Molybdenum |
Streckgrenze | 20.0 °C | 310 - 380 MPa Show Material materials with Streckgrenze of 310 - 380 MPa | |
Zugfestigkeit | 20.0 °C | 515 - 550 MPa Show Material materials with Zugfestigkeit of 515 - 550 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 4E-6 - 1.4E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 4E-6 - 1.4E-5 1/K | Typical for Molybdenum |
Schmelzpunkt | 2610 °C Show Material materials with Schmelzpunkt of 2610 °C | Typical for Molybdenum | |
Spezifische Wärmekapazität | 23.0 °C | 201 - 280 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 201 - 280 J/(kg·K) | Typical for Molybdenum |
Wärmeleitfähigkeit | 23.0 °C | 117 - 431 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 117 - 431 W/(m·K) | Typical for Molybdenum |
Chemical properties
Property | Value |
---|---|
Eisen | 0.01 % Show Material materials with Eisen of 0.01 % |
Kohlenstoff | 0.01 - 0.04 % Show Material materials with Kohlenstoff of 0.01 - 0.04 % |
Nickel | 5E-3 % Show Material materials with Nickel of 5E-3 % |
Sauerstoff | 0.03 % Show Material materials with Sauerstoff of 0.03 % |
Silizium | 5E-3 % Show Material materials with Silizium of 5E-3 % |
Stickstoff | 2E-3 % Show Material materials with Stickstoff of 2E-3 % |
Titan | 0.4 - 0.55 % Show Material materials with Titan of 0.4 - 0.55 % |