Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 12.7 g/cm³ Show Material materials with Dichte of 12.7 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Biegefestigkeit | 20.0 °C | 758 - 827 MPa Show Material materials with Biegefestigkeit of 758 - 827 MPa |
Härte, Rockwell B | 20.0 °C | 77 - 90 [-] Show Material materials with Härte, Rockwell B of 77 - 90 [-] |
Zugfestigkeit | 20.0 °C | 379 - 448 MPa Show Material materials with Zugfestigkeit of 379 - 448 MPa |
Elektrisch
Property | Value |
---|---|
Specific Electrical conductivity | 34 - 57 % IACS Show Material materials with Specific Electrical conductivity of 34 - 57 % IACS |
Chemical properties
Property | Value |
---|---|
Kupfer | 38 - 42 % Show Material materials with Kupfer of 38 - 42 % |