Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 13.7 g/cm³ Show Material materials with Dichte of 13.7 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Biegefestigkeit | 20.0 °C | 896 - 965 MPa Show Material materials with Biegefestigkeit of 896 - 965 MPa |
Härte, Rockwell B | 20.0 °C | 85 - 98 [-] Show Material materials with Härte, Rockwell B of 85 - 98 [-] |
Zugfestigkeit | 20.0 °C | 516 - 585 MPa Show Material materials with Zugfestigkeit of 516 - 585 MPa |
Elektrisch
Property | Value |
---|---|
Specific Electrical conductivity | 29 - 52 % IACS Show Material materials with Specific Electrical conductivity of 29 - 52 % IACS |
Chemical properties
Property | Value |
---|---|
Kupfer | 28 - 32 % Show Material materials with Kupfer of 28 - 32 % |