Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 14.3 g/cm³ Show Material materials with Dichte of 14.3 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Biegefestigkeit | 20.0 °C | 965 - 1034 MPa Show Material materials with Biegefestigkeit of 965 - 1034 MPa |
Härte, Rockwell B | 20.0 °C | 89 - 102 [-] Show Material materials with Härte, Rockwell B of 89 - 102 [-] |
Zugfestigkeit | 20.0 °C | 585 - 654 MPa Show Material materials with Zugfestigkeit of 585 - 654 MPa |
Elektrisch
Property | Value |
---|---|
Specific Electrical conductivity | 27 - 48 % IACS Show Material materials with Specific Electrical conductivity of 27 - 48 % IACS |
Chemical properties
Property | Value |
---|---|
Kupfer | 23 - 27 % Show Material materials with Kupfer of 23 - 27 % |